In vitro fracture and fatigue resistance of monolithic zirconia crowns fabricated by stereolithography

Zidi Zhai, Chao Qian, Ting Jiao, Jian Sun

The Journal of Prosthetic Dentistry · 2025

DOI: 10.1016/j.prosdent.2023.02.017 ↗

Kurz gefasst

Fachartikel in der Zeitschrift The Journal of Prosthetic Dentistry, 2025. Verfasst von Zidi Zhai und 3 weiteren Autor:innen. Beteiligte Einrichtung: Graduate student, Department of Prosthodontics, Shanghai Ninth People's Hospital, Shanghai Jiao Tong University School of Medicine; College of Stomat…. Hauptthemen laut MEDLINE: Zirconium, Crowns, Dental Prosthesis Design, Dental Restoration Failure. Die Arbeit wurde bisher 16-mal zitiert (Crossref) und nennt 32 Literaturangaben. Gefördert von: Fujian Medical University, Ministry of Science and Technology of the People's Republic of China, Shanghai City Science and Technology Commission.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

STATEMENT OF PROBLEM: Stereolithography has been used to print zirconia ceramic crowns with acceptable dimensional accuracy and fracture force. However, studies that compared the fatigue resistance of zirconia crowns fabricated by stereolithography are lacking. PURPOSE: The purpose of this in vitro study was to compare the fracture and fatigue resistance of monolithic zirconia crowns printed by stereolithography apparatus (SLA) and digital light processing (DLP) with those of zirconia crowns milled by computer numerical control (CNC). MATERIAL AND METHODS: A total of 120 crowns were fabricated (n=40/material) and underwent 0, 104, 105, or 106 dynamic loading cycles of 30 to 300 N in artificial saliva, followed by a static fracture loading test (n=10). After fracture, 1 crown from each group was selected for fractography analysis by scanning electron microscopy (SEM). Data were statistically analyzed through 2-way ANOVA and post hoc analysis for multiple comparisons (α=.05). RESULTS: The 2-way ANOVA results showed that the mean ±standard deviation force at fracture was the highest for CNC (before fatigue loading: 5154 ±568 N, 104: 5735 ±1231 N, 105: 5523 ±797 N, and 106: 6007 ±1258 N), followed by DLP (before fatigue loading: 3381 ±612 N, 104: 4046 ±1146 N, 105: 2929 ±559 N, and 106: 3223 ±739 N), and the lowest for SLA (before fatigue loading: 2956 ±598 N, 104: 2757 ±421 N, 105: 3326 ±391 N, and 106: 3103 ±246 N) (P .05). Fractography analysis showed that the number of arrest lines increased for crowns of all 3 materials. SEM images also showed the steps of SLA and DLP from their layer-by-layer printing and small cracks between layers of SLA after 106 loading cycles. CONCLUSIONS: The fracture force of monolithic zirconia crowns milled by CNC was significantly higher than that of zirconia crowns printed by stereolithography. Zirconia crowns printed by SLA and DLP could withstand typical clinical conditions, and their fracture and fatigue resistance exceeded the clinically estimated average occlusal forces.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

ZirconiumCrownsDental Prosthesis DesignDental Restoration FailureDental MaterialsComputer-Aided DesignDental Stress AnalysisIn Vitro TechniquesMaterials TestingMicroscopy, Electron, ScanningHumansPrinting, Three-DimensionalSurface Properties

Substanzen

Zirconiumzirconium oxideDental Materials

Autor:innen und Institutionen

  • Graduate student, Department of Prosthodontics, Shanghai Ninth People's Hospital, Shanghai Jiao Tong University School of Medicine; College of Stomatology, Shanghai Jiao Tong University; National Center for Stomatology;…
  • Senior Lecturer, Department of Prosthodontics, Shanghai Ninth People's Hospital, Shanghai Jiao Tong University School of Medicine; College of Stomatology, Shanghai Jiao Tong University; National Center for Stomatology;…
  • Professor, Department of Prosthodontics, Shanghai Ninth People's Hospital, Shanghai Jiao Tong University School of Medicine; College of Stomatology, Shanghai Jiao Tong University; National Center for Stomatology; Nation…

Förderung

  • Fujian Medical University
  • Ministry of Science and Technology of the People's Republic of China
  • Shanghai City Science and Technology Commission
  • National Key Research and Development Program of China

Zitieren

APA

Zhai, Z., Qian, C., Jiao, T., & Sun, J. (2025). In vitro fracture and fatigue resistance of monolithic zirconia crowns fabricated by stereolithography. The Journal of Prosthetic Dentistry. https://doi.org/10.1016/j.prosdent.2023.02.017

Vancouver

Zhai Z, Qian C, Jiao T, Sun J. In vitro fracture and fatigue resistance of monolithic zirconia crowns fabricated by stereolithography. The Journal of Prosthetic Dentistry. 2025. doi:10.1016/j.prosdent.2023.02.017

BibTeX
@article{Zhai2025,
  author = {Zhai, Zidi and Qian, Chao and Jiao, Ting and Sun, Jian},
  title = {In vitro fracture and fatigue resistance of monolithic zirconia crowns fabricated by stereolithography},
  journal = {The Journal of Prosthetic Dentistry},
  year = {2025},
  doi = {10.1016/j.prosdent.2023.02.017}
}
Kostenlos starten →