EUVIMEDEUVIMED entdecken
Crossref

Experimental Investigation of Wire EDM Parameters on Material Removal Rate for EN31 Alloy Steel

Anjan Kumar Kakati, Nayanjyoti Talukdar, Rajani Kant Baro

IOSR Journal of Mechanical and Civil Engineering · 2026-05 · 23 (5) · 46-57

DOI: 10.9790/1684-2305014657 ↗

Kurz gefasst

Fachartikel in der Zeitschrift IOSR Journal of Mechanical and Civil Engineering, 2026-05. Verfasst von Anjan Kumar Kakati und 2 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, material removal mechanism and process stability limits during wire electrical discharge machining (WEDM) of fully hardened EN31 die steel using a ∅ 0.25 mm zinc-coated brass wire have been investigated. A controlled parametric matrix was employed to evaluate the individual and synergistic effects of pulse-on time (Ton), pulse-off time (Toff), servo voltage (Sv), wire feed rate (Wf), wire tension (Wt) and wire polarity (Wp) to assess volumetric material removal rate (MRR), cutting speed and overall system operability. The experimental results indicate a significant dynamic variation of MRR by 18.3 times from 171.68 mm3 /min at low duty cycle (17.14%) to a maximum of 3149.08 mm3 /min at maximum duty cycle (45.45%). The scaling of performance is threshold dependent rather than linear. Above a critical energy threshold (𝑇on = 25 𝜇s, 𝑇off = 30 𝜇s) a strong localized thermal accumulation develops along the core of the traveling wire tool, leading to a sudden rupture of the wire. Further analysis isolates the influence of secondary non-electrical settings. Higher servo voltages (𝑆v = 30 V) and higher feed rates (𝑊f = 7 – 12 mm/min) promote a stable interelectrode gap that optimizes spark efficiency and debris evacuation. A practical manufacturing window is suggested for continuous industrial operations without wire failure at a duty cycle envelope of 38 - 40% (𝑇on = 22 – 23 𝜇s, 𝑇off = 33 – 5 𝜇s). Finally, a dual-pass machining strategy is presented to achieve maximum volume productivity while preserving high surface integrity for parts subjected to rolling contact fatigue because the high energy roughing operations produce a brittle recast layer (15–30 μm thick) on the sensitive EN31 surface.

Zitieren

APA

Kakati, A. K., Talukdar, N., & Baro, R. K. (2026). Experimental Investigation of Wire EDM Parameters on Material Removal Rate for EN31 Alloy Steel. IOSR Journal of Mechanical and Civil Engineering, 23(5), 46-57. https://doi.org/10.9790/1684-2305014657

Vancouver

Kakati AK, Talukdar N, Baro RK. Experimental Investigation of Wire EDM Parameters on Material Removal Rate for EN31 Alloy Steel. IOSR Journal of Mechanical and Civil Engineering. 2026;23(5):46-57. doi:10.9790/1684-2305014657

BibTeX
@article{Kakati2026,
  author = {Kakati, Anjan Kumar and Talukdar, Nayanjyoti and Baro, Rajani Kant},
  title = {Experimental Investigation of Wire EDM Parameters on Material Removal Rate for EN31 Alloy Steel},
  journal = {IOSR Journal of Mechanical and Civil Engineering},
  year = {2026},
  volume = {23},
  number = {5},
  pages = {46--57},
  doi = {10.9790/1684-2305014657}
}
Kostenlos starten →