Bond strength between layering ceramic and zirconia core: influence of various surface conditioning of zirconia

Abdulaziz A AlHelal, Syed Rashid Habib, Saleh Alyousef, Nawaf Alhamzah, Meshal Alqahtani, Abdulaziz Alqahtani

PeerJ · 2025

DOI: 10.7717/peerj.20480 ↗

Kurz gefasst

Fachartikel in der Zeitschrift PeerJ, 2025. Verfasst von Abdulaziz A AlHelal und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh, Saudi Arabia. Hauptthemen laut MEDLINE: Zirconium, Ceramics, Dental Bonding. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Ongoing Research Funding Program (ORF-2025-950), King Saud University, Riyadh, Saudi Arabia.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

It is recommended to apply various surface modification techniques to improve the mechanical and chemical interaction between zirconia core and veneering ceramic. Therefore, the objective of this in-vitro study was to evaluate and compare the effects of various surface treatments over the zirconia core on the shear bond strength (SBS) between layering ceramic and zirconia core.

Methods

A total of 90 zirconium oxide (Cercon, Degudent GmbH, Hanau-Wolfgang, Germany) specimens were prepared with standardized dimensions (10 mm × 10 mm × 5 mm). The specimens were randomly divided into six groups of 15 specimens each (Control group-no surface treatment; Sandblasting with 25 µm Al 2 O 3 ; Sandblasting with 50 µm Al 2 O 3 ; Sandblasting with 110 µm Al 2 O 3 ; Etching with hydrofluoric acid (9.5%); Surface treatment using Zirface (nano layer etching technology for enhanced bonding strength of zirconia). All specimens were veneered with fluorapatite glass-ceramic (5 mm × 5 mm × 5 mm) using a custom silicone mold, sintered in a calibrated porcelain furnace, and verified with a digital caliper. Following veneering, the samples were embedded in self-curing acrylic resin within polyvinyl chloride molds and immersed in distilled water at 37 °C for 24 hours to simulate intraoral conditions. Using universal testing machine, specimens were tested for SBS. Analysis of variance (ANOVA) and Tukey’s-test were used for statistical analysis ( P ≤ 0.05). Surface topography of the surfaces treated and after debonding were examined using scanning electron microscope (SEM) and failure mode of different groups was also noted.

Results

The application of Zirface to the zirconia core had the highest mean SBS value (26.56 ± 1.25 MPa), followed by the hydrofluoric acid only group (23.42 ± 0.94 MPa). The control group with no surface treatment showed the least SBS values. While the groups with surface treatments of 25 and 50 aluminum oxide (Al 2 O 3 ) sandblasting showed SBS values of 17.16 ± 0.48 and 18.06 ± 0.89, respectively, with no significant difference ( p > 0.05) between the SBS values of the two groups. However, the sandblasting with 110 Al 2 O 3 particles over the zirconia core surface showed higher SBS values (20.53 ± 1.14) as compared to the 25 and 50 Al 2 O 3 particles.

Conclusion

The study found that the shear bond strength between zirconia and veneering ceramic is significantly influenced by the surface treatment used, with nano-layer etching and hydrofluoric acid etching enhancing adhesion, and larger alumina particles enhancing bonding durability.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

ZirconiumCeramicsDental BondingSurface PropertiesShear StrengthMaterials TestingAluminum OxideIn Vitro TechniquesDental Stress Analysis

Stichwörter der Autor:innen

Bond strengthDental ceramicsLayering ceramicsShear bond strengthZirconiaZirconia core

Substanzen

Zirconiumzirconium oxideAluminum Oxide

Autor:innen und Institutionen

  • Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh, Saudi Arabia.
  • Dental Internship Program, College of Dentistry, King Saud University, Riyadh, Saudi Arabia.

Förderung

  • Ongoing Research Funding Program (ORF-2025-950), King Saud University, Riyadh, Saudi Arabia

Zitieren

APA

AlHelal, A. A., Habib, S. R., Alyousef, S., Alhamzah, N., Alqahtani, M., & Alqahtani, A. (2025). Bond strength between layering ceramic and zirconia core: influence of various surface conditioning of zirconia. PeerJ. https://doi.org/10.7717/peerj.20480

Vancouver

AlHelal AA, Habib SR, Alyousef S, Alhamzah N, Alqahtani M, Alqahtani A. Bond strength between layering ceramic and zirconia core: influence of various surface conditioning of zirconia. PeerJ. 2025. doi:10.7717/peerj.20480

BibTeX
@article{AlHelal2025,
  author = {AlHelal, Abdulaziz A and Habib, Syed Rashid and Alyousef, Saleh and Alhamzah, Nawaf and Alqahtani, Meshal and Alqahtani, Abdulaziz},
  title = {Bond strength between layering ceramic and zirconia core: influence of various surface conditioning of zirconia},
  journal = {PeerJ},
  year = {2025},
  doi = {10.7717/peerj.20480}
}
Kostenlos starten →