Fracture Resistance of MOD Cavities Restored with Short Fibre, Long Fibre, & Ribbond Reinforcements: An in-vitro Comparative Study

Gayatri H. Giramkar, Anu Narang, Santosh Kumar Singh, Shivani Rawat, Sadhvi Pateriya, Naman Keshwani

Journal of Recent Advances in Applied Sciences (pISSN 0970-1990) · 28.06.2026 · 41 · 1-7

DOI: 10.71393/5hft8114 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Recent Advances in Applied Sciences (pISSN 0970-1990), online erschienen am 28.06.2026. Verfasst von Gayatri H. Giramkar und 5 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Introduction

Mesio-occluso-distal (MOD) cavity preparations significantly weaken posterior teeth by reducing cuspal stiffness and increasing susceptibility to fracture. Fibre-reinforced composite systems have been introduced to enhance the mechanical performance and longevity of restorations. Aim & Objective: To compare the fracture resistance and failure patterns of MOD cavities restored with short fibre composite, long fibre reinforcement, and Ribbond reinforcement with those restored using conventional composite resin. Materials & Methods: Forty extracted human molars with standardized MOD cavity preparations were randomly allocated into four groups (n = 10 each): Group I (conventional composite), Group II (short fibre composite), Group III (long fibre reinforcement), and Group IV (Ribbond reinforcement). Following restoration, specimens underwent compressive loading in a universal testing machine until fracture. Fracture resistance was recorded in Newtons (N), and failure modes were classified as restorable or non-restorable. Data were analyzed using one-way ANOVA and Tukey’s post-hoc test.

Results

Fracture resistance differed significantly among the groups (F = 1357.26, p < 0.001). Group II showed the highest mean fracture resistance (1197.50 ± 15.14 N), followed by Group III (1037.50 ± 15.14 N), Group IV (956.30 ± 9.83 N), and Group I (787.00 ± 16.02 N). Compared with the control group, short fibre, long fibre, and Ribbond reinforcement increased fracture resistance by 52.2%, 31.8%, and 21.5%, respectively. Reinforced restorations also demonstrated a higher proportion of restorable fractures, with the short fibre group showing the most favorable failure pattern (80%).

Conclusion

Fibre reinforcement significantly improves fracture resistance and promotes more favorable failure modes in MOD restorations. Short fibre composite demonstrated the best overall performance.

Zitieren

APA

Giramkar, G. H., Narang, A., Singh, S. K., Rawat, S., Pateriya, S., & Keshwani, N. (2026). Fracture Resistance of MOD Cavities Restored with Short Fibre, Long Fibre, & Ribbond Reinforcements: An in-vitro Comparative Study. Journal of Recent Advances in Applied Sciences (pISSN 0970-1990), 41, 1-7. https://doi.org/10.71393/5hft8114

Vancouver

Giramkar GH, Narang A, Singh SK, Rawat S, Pateriya S, Keshwani N. Fracture Resistance of MOD Cavities Restored with Short Fibre, Long Fibre, & Ribbond Reinforcements: An in-vitro Comparative Study. Journal of Recent Advances in Applied Sciences (pISSN 0970-1990). 2026;41:1-7. doi:10.71393/5hft8114

BibTeX
@article{Giramkar2026,
  author = {Giramkar, Gayatri H. and Narang, Anu and Singh, Santosh Kumar and Rawat, Shivani and Pateriya, Sadhvi and Keshwani, Naman},
  title = {Fracture Resistance of MOD Cavities Restored with Short Fibre, Long Fibre, & Ribbond Reinforcements: An in-vitro Comparative Study},
  journal = {Journal of Recent Advances in Applied Sciences (pISSN 0970-1990)},
  year = {2026},
  volume = {41},
  pages = {1--7},
  doi = {10.71393/5hft8114}
}
Kostenlos starten →