Fracture Resistance of Class II MOD Cavities Restored by Direct and Indirect Techniques and Different Materials Combination

Vasiliki Tsertsidou, Petros Mourouzis iD, Dimitrios Dionysopoulos iD, Panagiotis Pandoleon, Kosmas Tolidis

Polymers · 15.08.2023 · 15 (16) · 3413

DOI: 10.3390/polym15163413 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 15.08.2023. Verfasst von Vasiliki Tsertsidou und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Dental Tissues Pathology and Therapeutics, Division of Operative Dentistry, Faculty of Dentistry, Aristotle University of Thessaloniki,…. Die Arbeit wurde bisher 34-mal zitiert (Crossref) und nennt 63 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study aimed to evaluate the fracture resistance of class II MOD cavities restored using different techniques and materials. Sixty extracted maxillary molars were selected and standardized class II MOD cavities were prepared using a custom-made paralleling device. The specimens were divided into four groups based on the restoration technique used: Group 1 (direct resin composite), Group 2 (short-fiber-reinforced composite resin), Group 3 (composite polyethylene fiber reinforcement), and Group 4 (CAD/CAM resin inlays). Fracture resistance was assessed for each group after thermocycling aging for 10,000 cycles. The mode of fracture was assigned to five types using Burke’s classification. To compare the fracture force among the tested materials, a paired sample t-test was performed. The significance level for each test was set at p < 0.05. Significant differences in fracture resistance were observed among the different restoration techniques. CAD/CAM inlays (2166 ± 615 N), short-fiber-reinforced composite resin (2471 ± 761 N), and composite polyethylene fiber reinforcement (1923 ± 492 N) showed superior fracture resistance compared to the group restored with direct resin composite (1242 ± 436 N). The conventional resin composite group exhibited the lowest mean fracture resistance. The choice of restoration material plays a critical role in the clinical survival of large MOD cavities. CAD/CAM inlays and fiber-reinforced composites offer improved fracture resistance, which is essential for long-term success in extensive restorations.

Schlagwörter

Stichwörter der Autor:innen

CAD/CAMcomposite resincrack propensityshort fibers

Autor:innen und Institutionen

  • Department of Dental Tissues Pathology and Therapeutics, Division of Operative Dentistry, Faculty of Dentistry, Aristotle University of Thessaloniki, 54124 Thessaloniki, Greece.
  • Department of Prosthodontics, Faculty of Dentistry, School of Health Sciences, Aristotle University of Thessaloniki, 54124 Thessaloniki, Greece.

ORCID-Profile: Petros Mourouzis, Dimitrios Dionysopoulos

Zitieren

APA

Tsertsidou, V., Mourouzis, P., Dionysopoulos, D., Pandoleon, P., & Tolidis, K. (2023). Fracture Resistance of Class II MOD Cavities Restored by Direct and Indirect Techniques and Different Materials Combination. Polymers, 15(16), 3413. https://doi.org/10.3390/polym15163413

Vancouver

Tsertsidou V, Mourouzis P, Dionysopoulos D, Pandoleon P, Tolidis K. Fracture Resistance of Class II MOD Cavities Restored by Direct and Indirect Techniques and Different Materials Combination. Polymers. 2023;15(16):3413. doi:10.3390/polym15163413

BibTeX
@article{Tsertsidou2023,
  author = {Tsertsidou, Vasiliki and Mourouzis, Petros and Dionysopoulos, Dimitrios and Pandoleon, Panagiotis and Tolidis, Kosmas},
  title = {Fracture Resistance of Class II MOD Cavities Restored by Direct and Indirect Techniques and Different Materials Combination},
  journal = {Polymers},
  year = {2023},
  volume = {15},
  number = {16},
  pages = {3413},
  doi = {10.3390/polym15163413}
}
Kostenlos starten →