Comparative Analysis of Fatigue Performance in Asphalt Concrete Modified with Nano-Alumina and Nano-Silica
Emerging Trends in Engineering and Sustainability · 31.03.2026 · 2 (1) · 1-12
DOI: 10.65505/etes-25-0019 ↗Kurz gefasst
Fachartikel in der Zeitschrift Emerging Trends in Engineering and Sustainability, online erschienen am 31.03.2026. Verfasst von Amjad H. Albayati und 2 weiteren Autor:innen.
Abstract (Originalsprache)
This comprehensive study undertakes a two-tiered comparative analysis to systematically evaluate the fatigue and cracking performance of a 40-50 penetration grade asphalt binder and its corresponding asphalt concrete mixtures, modified with varying dosages (2%, 4%, and 6% by binder weight) of Nano-Alumina (NA) and Nano-Silica (NS). The experimental methodology involved extensive binder-level testing, including the evaluation of physical properties (penetration, softening point, ductility), rheological behavior (Rotational Viscosity (RV)), and fatigue characteristics using the Superpave parameter G* sin δ and the advanced Linear Amplitude Sweep (LAS) test. Furthermore, compatibility was assessed via storage stability and Scanning Electron Microscopy (SEM). The research culminated in mixture-level performance evaluation using the Indirect Tensile Cracking Test (IDEAL-CT) to derive the Cracking Tolerance Index (CT-Index), Flexibility Index (FI), and Crack Resistance Index (CRI). The results confirmed that both nanomaterials significantly enhance binder stiffness and thermal stability. Nano-Alumina (NA) consistently induced the most profound stiffening effect, reflected by a major reduction in penetration. Rheological and LAS testing indicated that NA provides a stable and progressive, dose-proportional enhancement in fatigue life from 2% to 6%, attributed to the formation of a sustained nanoscale reinforcement network. Conversely, Nano-Silica (NS) exhibited a potent viscosity-building effect due to its high surface area, achieving superior initial cracking tolerance and fatigue life at low concentrations (2% to 4%). Crucially, the study identified a narrow optimal range for NS; concentrations at 6% led to an adverse reduction in fatigue resistance (G* sin δ increase) and diminished flexibility, suggesting a constraint imposed by excessive stiffening and potential particle agglomeration. Mixture-level IDEAL-CT results further validated these trends: NA offered a balanced overall contribution, maximizing the CT-Index at 6% and CRI at 4%, while NS yielded an exceptionally high CT- Index value at 2% but showed a decline in performance at higher contents. The overall findings recommend an optimal practical dosage of 2-4% for NS and 4-6% for NA, underscoring the necessity of material-specific optimization for achieving enhanced durability and fatigue life under repeated loading.
Zitieren
APA
Albayati, A. H., Al-Hamdou, A. M., & Wang, Y. (2026). Comparative Analysis of Fatigue Performance in Asphalt Concrete Modified with Nano-Alumina and Nano-Silica. Emerging Trends in Engineering and Sustainability, 2(1), 1-12. https://doi.org/10.65505/etes-25-0019
Vancouver
Albayati AH, Al-Hamdou AM, Wang Y. Comparative Analysis of Fatigue Performance in Asphalt Concrete Modified with Nano-Alumina and Nano-Silica. Emerging Trends in Engineering and Sustainability. 2026;2(1):1-12. doi:10.65505/etes-25-0019
BibTeX
@article{Albayati2026,
author = {Albayati, Amjad H. and Al-Hamdou, Ali M. and Wang, Yu},
title = {Comparative Analysis of Fatigue Performance in Asphalt Concrete Modified with Nano-Alumina and Nano-Silica},
journal = {Emerging Trends in Engineering and Sustainability},
year = {2026},
volume = {2},
number = {1},
pages = {1--12},
doi = {10.65505/etes-25-0019}
}
EUVIMED