EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of Steam-Treatment Duration on the Physical and Mechanical Properties of Three-Layer Betung Bamboo (Dendrocalamus asper) Plybamboo Board

Sena Maulana, Muhammad Saeful Fadlan, Muhammad Iqbal Maulana, Sarah Augustina, Byantara Darsan Purusatama, Muhammad Aizat Abd Ghani

Greensusmater · 09.11.2026 · 3 (2)

DOI: 10.62755/gsm.2026.12 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Greensusmater, online erschienen am 09.11.2026. Verfasst von Sena Maulana und 5 weiteren Autor:innen. Die Arbeit nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Betung bamboo (Dendrocalamus asper) is a fast-growing, carbon-storing lignocellulosic resource that can relieve harvesting pressure on tropical hardwood, but its high starch and extractive content impairs adhesion and weakens bonded bamboo panels. Steam treatment offers a solvent- and chemical-free route to degrade these components, yet the exposure time best suited to a three-layer, poly(vinyl acetate) (PVAc)-bonded plybamboo board (PBB) has not been established for this sheet-based, cross-laminated architecture. We manufactured cross-laminated PBB (30×30×1.5 cm) from betung slats steamed with saturated steam at 126 °C for 0, 30, 45, and 60 min and measured density, moisture content, water absorption, thickness swelling, delamination, and static bending properties parallel and perpendicular to the grain. A short 30 min treatment gave the best mechanical profile, raising density by 11%, lowering water absorption by 19% and thickness swelling by 42%, and increasing parallel-grain modulus of elasticity and rupture by 82% and 56% relative to the untreated control; perpendicular-grain bending was statistically unchanged. The stiffness gain persists after density normalisation: the density-normalised (specific) modulus rose 64%, and panel density explained only 40% of the cross-panel variance in modulus. Longer treatment continued to improve dimensional stability (thickness swelling down 65% at 60 min, significantly below the 30 min value, and delamination down 54%) but progressively lowered density and strength. Measured moisture contents were below the SNI 8032:2014 reference limit (≤14%), and parallel-grain bending strengths exceeded the SNI 01-5008.7-1999 reference value, but none reached the intended 0.7 g cm−3 target density, and modulus of elasticity and perpendicular-grain strength fell short of the structural thresholds. Within this green, water-only process panel densification and adhesive formulation and application warrant further investigation, indicating where future optimisation of sustainable plybamboo should be directed.

Zitieren

APA

Maulana, S., Fadlan, M. S., Maulana, M. I., Augustina, S., Purusatama, B. D., & Ghani, M. A. A. (2026). Effect of Steam-Treatment Duration on the Physical and Mechanical Properties of Three-Layer Betung Bamboo (Dendrocalamus asper) Plybamboo Board. Greensusmater, 3(2). https://doi.org/10.62755/gsm.2026.12

Vancouver

Maulana S, Fadlan MS, Maulana MI, Augustina S, Purusatama BD, Ghani MAA. Effect of Steam-Treatment Duration on the Physical and Mechanical Properties of Three-Layer Betung Bamboo (Dendrocalamus asper) Plybamboo Board. Greensusmater. 2026;3(2). doi:10.62755/gsm.2026.12

BibTeX
@article{Maulana2026,
  author = {Maulana, Sena and Fadlan, Muhammad Saeful and Maulana, Muhammad Iqbal and Augustina, Sarah and Purusatama, Byantara Darsan and Ghani, Muhammad Aizat Abd},
  title = {Effect of Steam-Treatment Duration on the Physical and Mechanical Properties of Three-Layer Betung Bamboo (Dendrocalamus asper) Plybamboo Board},
  journal = {Greensusmater},
  year = {2026},
  volume = {3},
  number = {2},
  doi = {10.62755/gsm.2026.12}
}
Kostenlos starten →