Fracture resistance of screw-retained implant crowns using different restorative materials

Sameer Chauhan

Bioinformation · 31.10.2026 · 22 (10) · 7188-7191

DOI: 10.6026/973206300227188 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bioinformation, online erschienen am 31.10.2026. Verfasst von Sameer Chauhan.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Screw-retained implant crowns require restorative materials with adequate fracture resistance and predictable failure behaviour for long-term clinical success. Therefore, it is of interest to evaluate the fracture resistance and failure modes of 40 crowns fabricated from metal-ceramic, monolithic zirconia, lithium disilicate and polymer-infiltrated ceramic network (PICN) (n = 10/group). After thermocycling and cyclic mechanical loading, specimens underwent fracture testing and microscopic failure analysis. Monolithic zirconia exhibited the highest fracture resistance, followed by metal-ceramic, lithium disilicate and PICN, with statistically significant differences between all groups. Thus, restorative material influences fracture resistance and failure patterns, supporting material selection according to anticipated occlusal loads and clinical requirements.

Zitieren

APA

Chauhan, S. (2026). Fracture resistance of screw-retained implant crowns using different restorative materials. Bioinformation, 22(10), 7188-7191. https://doi.org/10.6026/973206300227188

Vancouver

Chauhan S. Fracture resistance of screw-retained implant crowns using different restorative materials. Bioinformation. 2026;22(10):7188-7191. doi:10.6026/973206300227188

BibTeX
@article{Chauhan2026,
  author = {Chauhan, Sameer},
  title = {Fracture resistance of screw-retained implant crowns using different restorative materials},
  journal = {Bioinformation},
  year = {2026},
  volume = {22},
  number = {10},
  pages = {7188--7191},
  doi = {10.6026/973206300227188}
}
Kostenlos starten →