EUVIMEDEUVIMED entdecken
Crossref

Comparative evaluation of fracture strength of CAD/CAM anterior FPD framework made with zirconia and peek–an in-vitro study

Jeevitha Mani, Abraham Ponsekar, Anand S., Tharsan Pravin, Mithra R., Ajith Kumar

Avances en Biomédicina · 2026 · 14 (2) · 140-148

DOI: 10.53766/avanbio/2025.14.2.07 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Avances en Biomédicina, 2026. Verfasst von Jeevitha Mani und 5 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study aimed to comparatively evaluate the fracture strength of Computer Aided Designing, Computer Aided Manufacturing, 3-unit anterior Zirconia, and PEEK framework. A prefabricated prepared teeth model for 3-unit anterior FPD in relation to 21,22 & 23 was obtained and scanned using 3 Shape, Trios intraoral scanner, and a metallic die was milled using base metal alloy. The metallic die was scanned using the same Intraoral scanner (3 shape, Trios), and five 3-unit CAD/CAM Zirconia (Group A) and five 3-unit PEEK (Group B) frameworks were fabricated and cemented to the metallic die using resin cement. A universal testing machine was used for the fracture strength evaluation. The load was applied to the specimen at a crosshead speed of 0.5mm/min until catastrophic failure occurred. This was repeated for all the FPD frameworks, and the fracture strength mean value was recorded and statistically analyzed through an Unpaired Student t-test. The mean fracture strength of CAD/CAM Zirconia is 1862 N +18.8149 N, and the mean fracture strength of CAD/CAM PEEK is 2563 N +19.7231 N. The Fracture strength of CAD/CAM PEEK framework was higher than that of CAD/CAM Zirconia framework. The values were statistically significant by 1% (p value < 0.01). Since PEEK showed a significantly higher fracture strength value compared to Zirconia, it could be an alternative metal-free, esthetic material for replacing missing anterior teeth.

Zitieren

APA

Mani, J., Ponsekar, A., S., A., Pravin, T., R., M., & Kumar, A. (2026). Comparative evaluation of fracture strength of CAD/CAM anterior FPD framework made with zirconia and peek–an in-vitro study. Avances en Biomédicina, 14(2), 140-148. https://doi.org/10.53766/avanbio/2025.14.2.07

Vancouver

Mani J, Ponsekar A, S. A, Pravin T, R. M, Kumar A. Comparative evaluation of fracture strength of CAD/CAM anterior FPD framework made with zirconia and peek–an in-vitro study. Avances en Biomédicina. 2026;14(2):140-148. doi:10.53766/avanbio/2025.14.2.07

BibTeX
@article{Mani2026,
  author = {Mani, Jeevitha and Ponsekar, Abraham and S., Anand and Pravin, Tharsan and R., Mithra and Kumar, Ajith},
  title = {Comparative evaluation of fracture strength of CAD/CAM anterior FPD framework made with zirconia and peek–an in-vitro study},
  journal = {Avances en Biomédicina},
  year = {2026},
  volume = {14},
  number = {2},
  pages = {140--148},
  doi = {10.53766/avanbio/2025.14.2.07}
}
Kostenlos starten →