Comparative Evaluation of Shear Bond Strength of Glass Ionomer Cement, Resin-Modified Glass Ionomer Cement and Alkasite Restorative Material to Human Dentin: An In-Vitro Study
Academia Journal of Medicine · 13.02.2026 · 9 (1) · 52-55
DOI: 10.48165/ajm.2026.9.01.13 ↗Kurz gefasst
Fachartikel in der Zeitschrift Academia Journal of Medicine, online erschienen am 13.02.2026. Verfasst von Boris Saha und 5 weiteren Autor:innen.
Abstract (Originalsprache)
Background
Durable adhesion between restorative materials and dentin is essential for the longevity and clinical success of restorations. Conventional glass ionomer cement (GIC), resin-modified glass ionomer cement (RMGIC), and alkasite restorative materials are widely used because of their fluoride release, chemical bonding potential, and simplified clinical application; however, their comparative bonding performance remains inconclusive.
Aim
To compare the shear bond strength (SBS) of conventional GIC, RMGIC, and alkasite restorative material to human dentin. Materials and Methods: Thirty extracted human premolars were sectioned to expose flat mid-coronal dentin surfaces and randomly allocated into three groups (n = 10): Group I—conventional GIC, Group II—RMGIC, and Group III—alkasite restorative material. Restorations were placed according to manufacturers’ instructions using a standardized cylindrical mold. After storage in distilled water at 37 °C for 24 hours, specimens were subjected to shear bond strength testing using a universal testing machine at a cross-head speed of 1 mm/min. SBS values were calculated in megapascals (MPa) and statistically analyzed using one-way analysis of variance followed by Tukey’s post-hoc test (α = 0.05).
Results
Alkasite restorative material demonstrated the highest mean shear bond strength (14.06 ± 1.87 MPa), followed by RMGIC (11.52 ± 1.74 MPa) and conventional GIC (8.94 ± 1.58 MPa). The differences among the three groups were statistically significant (p < 0.001).
Conclusion
Within the limitations of this in-vitro study, alkasite restorative material exhibited superior bonding to dentin compared with both types of glass ionomer cements. Conventional GIC showed the lowest shear bond strength.
Zitieren
APA
Saha, B., Vardhana, B., Sarkar, D., Resende, E. V., Gill, S., & Shrivastava, N. (2026). Comparative Evaluation of Shear Bond Strength of Glass Ionomer Cement, Resin-Modified Glass Ionomer Cement and Alkasite Restorative Material to Human Dentin: An In-Vitro Study. Academia Journal of Medicine, 9(1), 52-55. https://doi.org/10.48165/ajm.2026.9.01.13
Vancouver
Saha B, Vardhana B, Sarkar D, Resende EV, Gill S, Shrivastava N. Comparative Evaluation of Shear Bond Strength of Glass Ionomer Cement, Resin-Modified Glass Ionomer Cement and Alkasite Restorative Material to Human Dentin: An In-Vitro Study. Academia Journal of Medicine. 2026;9(1):52-55. doi:10.48165/ajm.2026.9.01.13
BibTeX
@article{Saha2026,
author = {Saha, Boris and Vardhana, Bharath and Sarkar, Dipaneeta and Resende, Eloá Vieira and Gill, Shreya and Shrivastava, Neetu},
title = {Comparative Evaluation of Shear Bond Strength of Glass Ionomer Cement, Resin-Modified Glass Ionomer Cement and Alkasite Restorative Material to Human Dentin: An In-Vitro Study},
journal = {Academia Journal of Medicine},
year = {2026},
volume = {9},
number = {1},
pages = {52--55},
doi = {10.48165/ajm.2026.9.01.13}
}
EUVIMED