Comparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study
Applied Sciences · 01.06.2026 · 16 (11) · 5493
DOI: 10.3390/app16115493 ↗Kurz gefasst
Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 01.06.2026. Verfasst von Hanan Filemban und 6 weiteren Autor:innen. Die Arbeit nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
This in vitro study evaluated and compared the shear bond strength (SBS) of three restorative materials bonded to dentin: a glass hybrid ionomer (EQUIA Forte HT), a resin-modified glass ionomer (RIVA Light Cure), and a nanofilled composite resin (Filtek Z350 XT). Additionally, their modes of failure were assessed. Thirty extracted human teeth were prepared and randomly assigned to three groups (n = 10) by restorative material: Group 1: Filtek Z350 XT; Group 2: EQUIA Forte HT; Group 3: RIVA Light Cure. All materials were applied following manufacturer instructions. SBS testing used a universal testing machine, applying a load at the tooth–restoration interface at 1 mm/min until failure. SBS values were recorded in megapascals (MPa). Failure modes were examined under a stereomicroscope at 40× magnification. A one-way ANOVA compared mean SBS among groups, with post hoc tests for pairwise group comparisons.
Results
Filtek Z350 XT had the highest mean SBS (21 MPa), followed by RIVA Light Cure (7.5 MPa) and EQUIA Forte HT (7.2 MPa). One-way ANOVA indicated a statistically significant difference in SBS (p < 0.05). Post hoc analysis showed Filtek Z350 XT had significantly higher SBS than the glass ionomer-based materials, while EQUIA Forte HT and RIVA Light Cure did not differ significantly.
Conclusions
Filtek Z350 XT demonstrated significantly higher shear bond strength to dentin than the glass ionomer-based materials. No significant SBS difference was found between the resin-modified and hybrid glass ionomers.
Zitieren
APA
Filemban, H., Bawazir, M., Alothman, K. A., Turkestani, N. A., Merdad, Y. M., Hajjaj, M. S., & Alzahrani, S. J. (2026). Comparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study. Applied Sciences, 16(11), 5493. https://doi.org/10.3390/app16115493
Vancouver
Filemban H, Bawazir M, Alothman KA, Turkestani NA, Merdad YM, Hajjaj MS, et al. Comparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study. Applied Sciences. 2026;16(11):5493. doi:10.3390/app16115493
BibTeX
@article{Filemban2026,
author = {Filemban, Hanan and Bawazir, Marwa and Alothman, Khawlah A. and Turkestani, Najla Al and Merdad, Yasser M. and Hajjaj, Maher S. and Alzahrani, Saeed J.},
title = {Comparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study},
journal = {Applied Sciences},
year = {2026},
volume = {16},
number = {11},
pages = {5493},
doi = {10.3390/app16115493}
}
EUVIMED