Fachartikel in der Zeitschrift Indian Journal of Dental Research, 2023. Verfasst von J Dhivya Priya und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics and Crown and Bridge, CSI College of Dental Sciences and Research, The Tamil Nadu Dr. MGR Medical University, Madurai, T…. Hauptthemen laut MEDLINE: Flexural Strength, Polymethyl Methacrylate. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 17 Literaturangaben.
Abstract (Originalsprache)
Introduction
To compare the flexural strength of autopolymerizing poly methyl methacrylate resins (PMMA) resin, CAD/CAM milled PMMA and CAD/CAM milled poly ether ether ketone (PEEK) when used as provisional restorative materials for long span situations in full mouth rehabilitation after aging and thermocycling. Materials and Methods: Sixty samples (25 mm × 2 mm × 2 mm) were fabricated using autopolymerizing PMMA resin (GROUP I), CAD/CAM milled PMMA (GROUP II) and PEEK (GROUP III). The groups were subdivided into A and B and subjected to 7 days of aging and 500 cycles of thermocycling (subgroup A) and 14 days of aging and 1000 cycles of thermocycling (subgroup B), respectively, and flexural strength was evaluated using a three-point bend test. The data were analyzed with student t test and pair-wise comparison of mean values was done by ANOVA.
Results
The flexural strength of PEEK subjected to 7 days of aging and 500 cycles of thermocycling (III (A) - 6628.70 MPa) was the highest among all groups followed by PEEK subjected to 14 days of aging and 1000 cycles of thermocycling (III (B) - 3760.50 MPa).
Conclusion
The mean flexural strength of PEEK was statistically significant than the other two materials tested and hence can be recommended for use as a provisional restorative material for long span situations in full mouth rehabilitation. However, the mean flexural strength of PEEK reduced approximately by 44% when subjected to further aging.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Prosthodontics and Crown and Bridge, CSI College of Dental Sciences and Research, The Tamil Nadu Dr. MGR Medical University, Madurai, Tamil Nadu, India.
Zitieren
APA
Priya, J. D., Lambodharan, R., Balakrishnan, S., Muthukumar, R., Selvaraj, S., & Ramalingam, S. (2023). Effect of Aging and Thermocycling on Flexural Strength of PEEK as a Provisional Restoration for Full Mouth Rehabilitation – An in Vitro Study. Indian Journal of Dental Research. https://doi.org/10.4103/ijdr.ijdr_195_21
Vancouver
Priya JD, Lambodharan R, Balakrishnan S, Muthukumar R, Selvaraj S, Ramalingam S. Effect of Aging and Thermocycling on Flexural Strength of PEEK as a Provisional Restoration for Full Mouth Rehabilitation – An in Vitro Study. Indian Journal of Dental Research. 2023. doi:10.4103/ijdr.ijdr_195_21
BibTeX
@article{Priya2023,
author = {Priya, J Dhivya and Lambodharan, R and Balakrishnan, Sivasaranya and Muthukumar, R and Selvaraj, Sabarinathan and Ramalingam, Sridharan},
title = {Effect of Aging and Thermocycling on Flexural Strength of PEEK as a Provisional Restoration for Full Mouth Rehabilitation – An in Vitro Study},
journal = {Indian Journal of Dental Research},
year = {2023},
doi = {10.4103/ijdr.ijdr_195_21}
}
EUVIMED