EUVIMEDEUVIMED entdecken
Crossref

Residual monomer content of repair autopolymerizing resin after microwave postpolymerization treatment

Prince Kumar, Deepti Raghav, Sukant Sahoo, Devvrat Singh, Suraj Suvarna, Tamanna Chhabra

European Journal of Prosthodontics · 2014

DOI: 10.4103/2347-4610.122991 ↗

Kurz gefasst

Fachartikel in der Zeitschrift European Journal of Prosthodontics, 2014. Verfasst von Prince Kumar und 5 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 31 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Purpose

Acrylic resins are one of the extensively used materials in removable prosthodontics however; complete dentures are highly vulnerable to fracture after long periods of clinical use. The repair of fractured prosthesis can be accomplished using acrylic resins that are light polymerized, autopolymerized, heat polymerized or microwave polymerized.

Aim

To evaluate the residual monomer content of three different repair autoploymerising resins processed by two different polymerization techniques after microwave postpolymerization treatment. Materials and Methods: The study was executed with fabrication of a metal die and sixty test specimens of three different materials. The specimens were cured with conventional method and using pressure pot. After this the specimens were tested for residual monomer content using Fourier transform infrared spectroscopy. Results and Conclusion: Results confirmd that their residual monomer content decreased by subjecting them to another cycle of polymerization in microwave at 550 watts for 3 minutes.

Zitieren

APA

Kumar, P., Raghav, D., Sahoo, S., Singh, D., Suvarna, S., & Chhabra, T. (2014). Residual monomer content of repair autopolymerizing resin after microwave postpolymerization treatment. European Journal of Prosthodontics. https://doi.org/10.4103/2347-4610.122991

Vancouver

Kumar P, Raghav D, Sahoo S, Singh D, Suvarna S, Chhabra T. Residual monomer content of repair autopolymerizing resin after microwave postpolymerization treatment. European Journal of Prosthodontics. 2014. doi:10.4103/2347-4610.122991

BibTeX
@article{Kumar2014,
  author = {Kumar, Prince and Raghav, Deepti and Sahoo, Sukant and Singh, Devvrat and Suvarna, Suraj and Chhabra, Tamanna},
  title = {Residual monomer content of repair autopolymerizing resin after microwave postpolymerization treatment},
  journal = {European Journal of Prosthodontics},
  year = {2014},
  doi = {10.4103/2347-4610.122991}
}
Kostenlos starten →