EUVIMEDEUVIMED entdecken
Crossref

Sustainable Ambient-Air Cu-Cu Wedge Bonding via Cu-Selective Ultrathin Passivation

Oliver Chyan, Shyam Muralidharan Nair, Duwage Anushka Sandaruwan Perera, Wonbong Choi

IMAPSource Proceedings · 26.10.2026 · 2026 (Symposium)

DOI: 10.4071/001c.173037 ↗

Kurz gefasst

Fachartikel in der Zeitschrift IMAPSource Proceedings, online erschienen am 26.10.2026. Verfasst von Oliver Chyan und 3 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Despite advances in 2.5D and 3D packaging, wire bonding remains the most widely used interconnection method in the semiconductor industry. Direct copper-to-copper (Cu-Cu) wedge bonding is highly valued in IC packaging due to its excellent electrical and thermal properties and lower material cost compared to gold (Au). However, its industrial use is limited because bare Cu surfaces oxidize rapidly at typical assembly temperatures (198-200 °C), forming a native Cu oxide barrier that causes widespread non-stick-on-lead (NSOL) failures. Traditional solutions involve expensive silver (Ag) finishes or a reducing forming-gas atmosphere (95% N2, 5% H2), both of which increase cost, complexity, and environmental concerns. This study presents a sustainable, precious-metal-free, and forming-gas-free alternative by applying an ultrathin (12-20 nm) Cu-selective passivation layer as a thermal shield during wire bonding. Building on previous passivation studies focused on bimetallic systems such as aluminum (Al) and palladium-coated copper (PCC) wires, this work investigates true monometallic Cu-Cu wedge bonding using 33μm bare Cu wire. The non-passivated Cu leadframe showed 100% failure at lower bonding power [220-230 Ultrasonic Power (US)], with inconsistent adhesion and high pull-strength variability at higher power ranges. In contrast, the passivated leadframe achieved consistent bonding yield across all power levels, with stable pull strength of 3.0-5.0 gf at 220-230 US, 2.0-6.0 gf at 300 US, and 3.0-6.0 gf at 400 US. Post-bonding analysis confirmed the passivation remained chemically stable at 200 °C for 10 minutes, suppressing 60-70% of Cu-oxide growth. Post-pull test failure analysis further confirmed the mechanical integrity of the Cu-Cu interface, with failures primarily occurring as cohesive wire-neck breaks while the second wedge bond remained intact. These results demonstrate a scalable and eco-friendly alternative to traditional Ag-plated leadframes and costly PCC wires, aligning metallurgical reliability with environmental sustainability for next-generation microelectronics packaging.

Zitieren

APA

Chyan, O., Nair, S. M., Perera, D. A. S., & Choi, W. (2026). Sustainable Ambient-Air Cu-Cu Wedge Bonding via Cu-Selective Ultrathin Passivation. IMAPSource Proceedings, 2026(Symposium). https://doi.org/10.4071/001c.173037

Vancouver

Chyan O, Nair SM, Perera DAS, Choi W. Sustainable Ambient-Air Cu-Cu Wedge Bonding via Cu-Selective Ultrathin Passivation. IMAPSource Proceedings. 2026;2026(Symposium). doi:10.4071/001c.173037

BibTeX
@article{Chyan2026,
  author = {Chyan, Oliver and Nair, Shyam Muralidharan and Perera, Duwage Anushka Sandaruwan and Choi, Wonbong},
  title = {Sustainable Ambient-Air Cu-Cu Wedge Bonding via Cu-Selective Ultrathin Passivation},
  journal = {IMAPSource Proceedings},
  year = {2026},
  volume = {2026},
  number = {Symposium},
  doi = {10.4071/001c.173037}
}
Kostenlos starten →