Comparison of fracture strength after thermo-mechanical aging between provisional crowns made with CAD/CAM and conventional method

Tanapon Reeponmaha iD, Onauma Angwaravong iD, Thidarat Angwarawong iD

The Journal of Advanced Prosthodontics · 2020 · 12 (4) · 218

DOI: 10.4047/jap.2020.12.4.218 ↗

Kurz gefasst

Fachartikel in der Zeitschrift The Journal of Advanced Prosthodontics, 2020. Verfasst von Tanapon Reeponmaha und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand. Die Arbeit wurde bisher 77-mal zitiert (Crossref) und nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0). Gefördert von: Khon Kaen University.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

PURPOSE: The objectives of this study were to evaluate the fracture strength and fracture patterns of provisional crowns fabricated from different materials and techniques after receiving stress from a simulated oral condition. MATERIALS AND METHODS: A monomethacrylate-based resin (Unifast Trad) and a bis-acryl-based (Protemp 4) resin were used to fabricate provisional crowns using conventional direct technique. A milled monomethacrylate resin (Brylic Solid) and a 3D-printed bis-acrylate resin (Freeprint Temp) were chosen to fabricate provisional crowns using the CAD/CAM process. All cemented provisional crowns (n=10/group) were subjected to thermal cycling (5,000 cycles at 5°-55℃) and cyclic occlusal load (100 N at 4 Hz for 100,000 cycles). Maximum force at fracture was tested using a universal testing machine. RESULTS: Maximum force at fracture (mean ± SD, N) of each group was 657.87 ± 82.84 for Unifast Trad, 1125.94 ± 168.07 for Protemp4, 953.60 ± 58.88 for Brylic Solid, and 1004.19 ± 122.18 for Freeprint Temp. One-way ANOVA with Tamhane post hoc test showed that the fracture strength of Unifast Trad was statistically significantly lower than others (P

Schlagwörter

Stichwörter der Autor:innen

3D printingComputer-aided design/computer-aided manufacturing (CAD/CAM)Fracture strengthProvisional restorations

Autor:innen und Institutionen

  • Department of Prosthodontics, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand.
  • Division of Pediatric Dentistry, Department of Preventive Dentistry, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand.

ORCID-Profile: Tanapon Reeponmaha, Onauma Angwaravong, Thidarat Angwarawong

Förderung

  • Khon Kaen University

Zitieren

APA

Reeponmaha, T., Angwaravong, O., & Angwarawong, T. (2020). Comparison of fracture strength after thermo-mechanical aging between provisional crowns made with CAD/CAM and conventional method. The Journal of Advanced Prosthodontics, 12(4), 218. https://doi.org/10.4047/jap.2020.12.4.218

Vancouver

Reeponmaha T, Angwaravong O, Angwarawong T. Comparison of fracture strength after thermo-mechanical aging between provisional crowns made with CAD/CAM and conventional method. The Journal of Advanced Prosthodontics. 2020;12(4):218. doi:10.4047/jap.2020.12.4.218

BibTeX
@article{Reeponmaha2020,
  author = {Reeponmaha, Tanapon and Angwaravong, Onauma and Angwarawong, Thidarat},
  title = {Comparison of fracture strength after thermo-mechanical aging between provisional crowns made with CAD/CAM and conventional method},
  journal = {The Journal of Advanced Prosthodontics},
  year = {2020},
  volume = {12},
  number = {4},
  pages = {218},
  doi = {10.4047/jap.2020.12.4.218}
}
Kostenlos starten →