Phase 2 and RDL Adhesion Measurement Test Methods for WLPs

Steven R. Martell, Lisa Chen, Iqbal Mokhtar, Rowling Luo, Gilad Nave, Masahiro Tsuriya

Wafer-Level Packaging Symposium · 2026-02 · 22 (1) · 5-7

DOI: 10.37665/wauuibm61292 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Wafer-Level Packaging Symposium, 2026-02. Verfasst von Steven R. Martell und 5 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

At WLPS 2023 and 2024 the initial and follow-up work done under Phase 1 of an iNEMI project was presented with plans for the next steps in the investigation of RDL (redistribution layers) adhesion measurements. This presentation will cover the Phase 2 plan and any initial results of the RDL Adhesion Project, plus the new SEMI Guideline for Peel Test Method. As mentioned previously, in 2019 iNEMI published a technology roadmap that included challenges and unknowns. One of those challenges was determining the actual adhesion strength of RDLs to materials used within WLPs (wafer level packages), PLP (panel level packages), and on advanced substrates with fine pitch traces. These fine lines are typically exposed to the manufacturing environment, which can result in the degradation of adhesion between the RDL traces and other materials, such as the encapsulant, die, and other dielectrics. It has been assumed that the adhesion properties measured with an older IPC test method, IPC-TM-650, for Cu traces 1mm (1000μm) and larger would also apply to thinner and fine traces 20μm wide and smaller, however from the data collected so far this appears to be a false assumption. There were concerns about characterizing the adhesion strength at the relevant length and small scales needed to duplicate WLP applications. The test method(s) developed have indicated that these smaller features are affected by flaws and features that are not significant in larger trace patterns. In addition, the traditional test method(s) such as peel and shear, do have challenges, including, but not limited to, the risk of trace breakage and tool load detection limitations for traces below 20μm. This will be the third presentation at WLPS on the work, plans, and results for the iNEMI RDL Adhesion Project. Phase 1 has been completed and has led to the creation of a SEMI Guideline for Peel Testing of RDL structures. The status and general outline of the test method will be discussed and presented. Phase 2 of the iNEMI RDL Adhesion project has begun and will investigate smaller trace widths/structures, other material combinations beyond copper traces to ABF substrates, and environment affects and/or degradation of the adhesion strength.

Zitieren

APA

Martell, S. R., Chen, L., Mokhtar, I., Luo, R., Nave, G., & Tsuriya, M. (2026). Phase 2 and RDL Adhesion Measurement Test Methods for WLPs. Wafer-Level Packaging Symposium, 22(1), 5-7. https://doi.org/10.37665/wauuibm61292

Vancouver

Martell SR, Chen L, Mokhtar I, Luo R, Nave G, Tsuriya M. Phase 2 and RDL Adhesion Measurement Test Methods for WLPs. Wafer-Level Packaging Symposium. 2026;22(1):5-7. doi:10.37665/wauuibm61292

BibTeX
@article{Martell2026,
  author = {Martell, Steven R. and Chen, Lisa and Mokhtar, Iqbal and Luo, Rowling and Nave, Gilad and Tsuriya, Masahiro},
  title = {Phase 2 and RDL Adhesion Measurement Test Methods for WLPs},
  journal = {Wafer-Level Packaging Symposium},
  year = {2026},
  volume = {22},
  number = {1},
  pages = {5--7},
  doi = {10.37665/wauuibm61292}
}
Kostenlos starten →