Dielectric properties of 2 inch polycrystalline diamond wafer at frequencies ranging from 10 to 330 GHz
Japanese Journal of Applied Physics · 01.11.2025 · 64 (11) · 118001
DOI: 10.35848/1347-4065/ae17fc ↗Kurz gefasst
Fachartikel in der Zeitschrift Japanese Journal of Applied Physics, online erschienen am 07.11.2025. Verfasst von Yoshiyuki Yanagimoto und 2 weiteren Autor:innen. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 12 Literaturangaben.
Abstract (Originalsprache)
Relative permittivity and dielectric losses (loss tangents) of a 2 inch polycrystalline diamond wafer are measured over frequency range of 10–330 GHz. Loss tangent values as low as 2 × 10 −6 –3.5 × 10 −5 are obtained across the entire range and are found to decrease with increasing the frequency in the 220–330 GHz band, likely due to conductivity originating from non-diamond phases. Diamond-based materials are promising candidates for 6G communication technologies.
Zitieren
APA
Yanagimoto, Y., Yanagimoto, S., & Koide, Y. (2025). Dielectric properties of 2 inch polycrystalline diamond wafer at frequencies ranging from 10 to 330 GHz. Japanese Journal of Applied Physics, 64(11), 118001. https://doi.org/10.35848/1347-4065/ae17fc
Vancouver
Yanagimoto Y, Yanagimoto S, Koide Y. Dielectric properties of 2 inch polycrystalline diamond wafer at frequencies ranging from 10 to 330 GHz. Japanese Journal of Applied Physics. 2025;64(11):118001. doi:10.35848/1347-4065/ae17fc
BibTeX
@article{Yanagimoto2025,
author = {Yanagimoto, Yoshiyuki and Yanagimoto, Shana and Koide, Yasuo},
title = {Dielectric properties of 2 inch polycrystalline diamond wafer at frequencies ranging from 10 to 330 GHz},
journal = {Japanese Journal of Applied Physics},
year = {2025},
volume = {64},
number = {11},
pages = {118001},
doi = {10.35848/1347-4065/ae17fc}
}
EUVIMED