EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Synthesis of Homogeneously {100}-Textured 3-Inch Free-Standing Diamond Wafer

Jing Zhang, Stephan Handschuh-Wang iD, Zhicheng Xing, Tao Wang iD

Materials · 04.06.2026 · 19 (11) · 2398

DOI: 10.3390/ma19112398 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 04.06.2026. Verfasst von Jing Zhang und 3 weiteren Autor:innen. Beteiligte Einrichtung: School of Integrated Circuits, Shenzhen Polytechnic University, Shenzhen 518055, China. Die Arbeit nennt 57 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Shenzhen Science and Technology Program.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

A two-step growth process was developed to fabricate a 3-inch homogeneously {100}-textured free-standing diamond wafer by microwave plasma enhanced chemical vapor deposition (MPCVD). The sequential growth process is based on a change in the growth parameter α, which is given by the growth rates on {100} and {111} facets, α = 3·(V100/V111). Initial growth was executed with nitrogen addition, yielding an α value close to 3 for evolutionary selection of the (100) face, followed by cessation of nitrogen addition to yield a lower α value. A homogeneously grown {100}-textured diamond over an area of ca. 175 cm2 with a thickness ≥ 0.8 mm was obtained after 196 h growth. The diamond growth rate was 4.0–5.5 µm/h, which is four times higher than the conventional growth of oriented diamond. This was substantiated by optical microscopy, Raman spectroscopy, and XRD analysis. The large crystal size of 210 ± 60 µm has been assigned to the second growth step, where growth is preferentially in the direction. The homogeneous {100} texture and the large crystal size are conducive to achieving high thermal conductivity, as the in-plane thermal conductivity of the polycrystalline diamond wafer was increased from ca. 850 W/(mK) to 1125 W/(mK).

Schlagwörter

Stichwörter der Autor:innen

MPCVDdiamondlarge areanitrogen addition{100}-textured microcrystalline diamond

Autor:innen und Institutionen

  • School of Integrated Circuits, Shenzhen Polytechnic University, Shenzhen 518055, China.
  • Glory Zenith Jinxel Semiconductor Co., Ltd., Shenzhen 518110, China.
  • College of New Materials and New Energies, Shenzhen Technology University, Shenzhen 518118, China.

ORCID-Profile: Stephan Handschuh-Wang, Tao Wang

Förderung

  • National Natural Science Foundation of China
  • Shenzhen Science and Technology Program

Zitieren

APA

Zhang, J., Handschuh-Wang, S., Xing, Z., & Wang, T. (2026). Synthesis of Homogeneously {100}-Textured 3-Inch Free-Standing Diamond Wafer. Materials, 19(11), 2398. https://doi.org/10.3390/ma19112398

Vancouver

Zhang J, Handschuh-Wang S, Xing Z, Wang T. Synthesis of Homogeneously {100}-Textured 3-Inch Free-Standing Diamond Wafer. Materials. 2026;19(11):2398. doi:10.3390/ma19112398

BibTeX
@article{Zhang2026,
  author = {Zhang, Jing and Handschuh-Wang, Stephan and Xing, Zhicheng and Wang, Tao},
  title = {Synthesis of Homogeneously 100-Textured 3-Inch Free-Standing Diamond Wafer},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {11},
  pages = {2398},
  doi = {10.3390/ma19112398}
}