Mechanisms of Metal Particle Release from Pipe Scales in Ductile Iron Water Supply Pipelines: Control by Water Quality Parameters
Water · 04.05.2026 · 18 (9) · 1101
DOI: 10.3390/w18091101 ↗Kurz gefasst
Fachartikel in der Zeitschrift Water, online erschienen am 04.05.2026. Verfasst von Yu Chang und 4 weiteren Autor:innen. Die Arbeit nennt 30 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, National Key Research and Development Program of China.
Abstract (Originalsprache)
To clarify the control mechanism of water quality parameters on metal particle release from pipe scales in aging ductile iron water supply pipelines (service life > 20 years), this study conducted single-factor experiments to explore the effects of pH, temperature, concentration of humic acid (HA) and Mn2+ on Fe, Mn, and Al particle release. Combined with inductively coupled plasma optical emission spectrometry (ICP-OES) for quantitative detection, first-order/second-order kinetic fitting, and X-ray diffraction (XRD) and scanning electron microscopy-energy dispersive spectrometry (SEM-EDS) characterization, the results showed that an increase in temperature generally promoted the aggregation and sedimentation of metal particles, among which Fe and Mn particles were more sensitive to temperature changes. pH affected the sedimentation process by controlling metal ion speciation and particle surface charge: low pH significantly accelerated pipe scale dissolution, while weakly alkaline conditions prolonged particle suspension time. Low-concentration HA (0.5 mg/L) promoted particle dissolution, whereas high-concentration HA (1.0–2.0 mg/L) extended particle retention time through surface coating. Mn2+ concentration exhibited an obvious concentration-dependent effect: the range of 20–50 μg/L enhanced particle suspension stability, while 80–100 μg/L accelerated particle aggregation and sedimentation. The pipe scales mainly consisted of Fe3O4, Fe2O3, Mn3O4, and Al2O3, with metal release regulated by the “element complexation–particle aggregation–crystal growth” pathway. Particle sedimentation followed first-order kinetics. Controlling pH at 7.0, temperature < 30 °C, and reducing HA/Mn2+ concentrations effectively weakened metal particle migration. This study reveals the coupled effect mechanism of water quality parameters, providing theoretical and technical support for optimizing water quality control and solving the “yellow water” problem.
Förderung
- National Natural Science Foundation of China
- National Key Research and Development Program of China
Zitieren
APA
Chang, Y., Fang, M., Lu, Q., Zhang, D., & Li, W. (2026). Mechanisms of Metal Particle Release from Pipe Scales in Ductile Iron Water Supply Pipelines: Control by Water Quality Parameters. Water, 18(9), 1101. https://doi.org/10.3390/w18091101
Vancouver
Chang Y, Fang M, Lu Q, Zhang D, Li W. Mechanisms of Metal Particle Release from Pipe Scales in Ductile Iron Water Supply Pipelines: Control by Water Quality Parameters. Water. 2026;18(9):1101. doi:10.3390/w18091101
BibTeX
@article{Chang2026,
author = {Chang, Yu and Fang, Menghao and Lu, Qing and Zhang, Dawei and Li, Weiying},
title = {Mechanisms of Metal Particle Release from Pipe Scales in Ductile Iron Water Supply Pipelines: Control by Water Quality Parameters},
journal = {Water},
year = {2026},
volume = {18},
number = {9},
pages = {1101},
doi = {10.3390/w18091101}
}