Fachartikel in der Zeitschrift Sustainability, online erschienen am 16.11.2026. Verfasst von Juan Hou und 2 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Science and Technology Department of Qinghai Province, China Scholarship Council.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The stability of waste containment facilities is critical for protecting the environment and contributing to sustainability, which is highly reliant on the interfacial strength of the composite liners consisting of a layer of geomembrane (GM) and a layer of geosynthetic clay liner (GCL). This study investigated the shear behavior of the GM–GCL interface with 3D-printed embossed textured geomembranes (3D-GMTEs) using large-scale direct shear tests under normal stresses of 100, 200, and 400 kPa. The asperity height, diameter, and spacing of the 3D-GMTEs were varied independently to evaluate their effects on interfacial shear strength. The 3D-GMTE–GCL interface showed similar overall shear stress–displacement responses to those of the commercial GMTE–GCL interface, but its large-displacement strengths were higher. The results show that, at 200 kPa, increasing asperity height from 0.5 mm to 1.0 mm increased the peak and large-displacement strengths by approximately 311% and 220%, respectively. The diameter associated with the highest peak and large-displacement strengths was 2 mm at 100 kPa and 3 mm at 200 and 400 kPa, whereas increasing asperity spacing from 4 mm to 16 mm consistently reduced shear strength. As asperity height increased from 0.5 mm to 1.5 mm, the peak and large-displacement friction angles increased from 9° and 6° to 34° and 20°, respectively. At 400 kPa, all interfaces remained compressive, with a final compression of 0.72 mm for the reference geometry. Post-shear photographs provided qualitative evidence of asperity deformation, localized penetration, fiber disturbance, bentonite extrusion, and shear striations. These findings establish a fundamental relationship between asperity-scale geometry and GMTE–GCL interface performance, providing mechanistic insights for the rational design of reliability, protecting the surrounding environment from waste contamination, and contributing to sustainability.

Förderung

  • National Natural Science Foundation of China
  • Science and Technology Department of Qinghai Province
  • China Scholarship Council

Zitieren

APA

Hou, J., Lu, S., & Xie, X. (2026). Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface. Sustainability, 18(22), 11673. https://doi.org/10.3390/su182211673

Vancouver

Hou J, Lu S, Xie X. Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface. Sustainability. 2026;18(22):11673. doi:10.3390/su182211673

BibTeX
@article{Hou2026,
  author = {Hou, Juan and Lu, Shen and Xie, Xuelei},
  title = {Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface},
  journal = {Sustainability},
  year = {2026},
  volume = {18},
  number = {22},
  pages = {11673},
  doi = {10.3390/su182211673}
}
Kostenlos starten →