Fachartikel in der Zeitschrift Solar, online erschienen am 18.05.2026. Verfasst von Wolfram Witte und 3 weiteren Autor:innen. Die Arbeit nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: German Federal Ministry for Economic Affairs and Energy, German Federal Ministry for Economic Affairs and Climate Action, European Union.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Chalcopyrite-based thin-film solar cells have great potential for various applications, such as top or bottom cells in tandem devices, in addition to their use as standard single-junction modules due to their tuneable bandgap energy. A bandgap energy Eg > 1.5 eV should be targeted to realize a wide-bandgap top cell, e.g., by increasing the [Ga]/([Ga] + [In]) (GGI) ratio in Cu(In,Ga)Se2 (CIGS) cells to the range of 0.7–1. A second approach is targeting the second theoretical efficiency maximum at a little lower Eg = 1.34 eV with a GGI around 0.6 for high-efficiency single-junction applications with reduced electrical losses. An industry-relevant (Ag,Cu)(In,Ga)Se2 (ACIGS) co-evaporation process for wide-bandgap cells fabricated with GGI ratios above 0.6, with moderate [Ag]/([Ag] + [Cu]) (AAC) ratios < 0.1 and in-line RbF-PDT, was established on molybdenum-coated soda-lime glass substrates. Both measures, Ag alloying and RbF-PDT, can increase power conversion efficiency (PCE) mainly due to improved open-circuit voltage (VOC). In addition, Ag addition can increase fill factor (FF), leading to an increase in the PCE for cells with GGI > 0.6 compared to Ag-free reference cells. (Zn,Mg)O, either with a [Mg]/([Mg] + [Zn]) ratio of 0.15 or 0.25, is a good option as high-resistive layer replacing the commonly used i-ZnO in combination with a CdS buffer. Our best ACIGS wide-bandgap solar cells with RbF-PDT and Zn0.85Mg0.15O (without anti-reflective coating (ARC)) from various experimental campaigns show a PCE of 12.7% (Eg = 1.50 eV), and with a slightly reduced Eg of 1.45 eV a PCE of 15.5%, with VOC of 933 mV (VOC deficit of 517 mV), and a good FF of 73.2%. In the case when the bandgap is significantly lowered to 1.34 eV (GGI = 0.61), to the second theoretical efficiency maximum, we achieved a PCE of 18.2% with ARC for an Ag-free CIGS cell with RbF-PDT. For this cell with a CdS/i-ZnO buffer system the VOC deficit is 480 mV, and the FF is 78.1%.

Förderung

  • German Federal Ministry for Economic Affairs and Energy
  • German Federal Ministry for Economic Affairs and Climate Action
  • European Union

Zitieren

APA

Witte, W., Gutzler, R., Paetel, S., & Hariskos, D. (2026). Measures to Improve Wide-Bandgap Cu(In,Ga)Se2 Solar Cells by Industry-Relevant In-Line Co-Evaporation. Solar, 6(3), 27. https://doi.org/10.3390/solar6030027

Vancouver

Witte W, Gutzler R, Paetel S, Hariskos D. Measures to Improve Wide-Bandgap Cu(In,Ga)Se2 Solar Cells by Industry-Relevant In-Line Co-Evaporation. Solar. 2026;6(3):27. doi:10.3390/solar6030027

BibTeX
@article{Witte2026,
  author = {Witte, Wolfram and Gutzler, Rico and Paetel, Stefan and Hariskos, Dimitrios},
  title = {Measures to Improve Wide-Bandgap Cu(In,Ga)Se2 Solar Cells by Industry-Relevant In-Line Co-Evaporation},
  journal = {Solar},
  year = {2026},
  volume = {6},
  number = {3},
  pages = {27},
  doi = {10.3390/solar6030027}
}
Kostenlos starten →