EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Mechanical Reinforcement and Early-Stage Deterioration of Cellulose Nanocrystal-Reinforced Isosorbide-Based Polycarbonate Nanocomposites Under Humid Soil Exposure

Yuli Nurul Maulida iD, Ellana Nabilah Nur Averina Ansar iD, Merreta Noorenza Biutty, PilHo Huh iD, Seong Il Yoo

Polymers · 05.11.2026 · 18 (21) · 2751

DOI: 10.3390/polym18212751 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 05.11.2026. Verfasst von Yuli Nurul Maulida und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Polymer Engineering, Pukyong National University, Busan 48547, Republic of Korea. Die Arbeit nennt 41 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Ministry of Trade, Industry and Energy, Pukyong National University.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Recently, the development of biomass-based polymers has attracted a great deal of attention as a sustainable alternative to petroleum-based plastics. However, the relatively limited mechanical properties of these bio-derived polymers often require reinforcement through the inclusion of nanofillers, while the environmental durability of such nanocomposites remains insufficiently understood. In this regard, we prepared nanocomposites composed of isosorbide-based polycarbonate (ISB-PC) and surface-modified cellulose nanocrystals (CNCs), and examined the effect of nanofillers on the mechanical properties and their retention under humid soil exposure. Interestingly, the initial reinforcement effect provided by CNCs rapidly decreased during the early stage of exposure, and the mechanical properties of the ISB-PC composites eventually converged toward those of pristine ISB-PC within a relatively short time. Based on the time-dependent changes in mechanical properties and mass loss, we propose that the mechanical deterioration was associated with physical changes in the polymer matrix, accompanied by the formation of macroscale cavities within the films. Our results suggest that initial reinforcement does not necessarily ensure sustained mechanical performance under humid soil exposure.

Schlagwörter

Stichwörter der Autor:innen

cellulose nanocrystals (CNCs)isosorbide-based polycarbonate (ISB-PC)mechanical propertynanocompositessoil burial

Autor:innen und Institutionen

  • Department of Polymer Engineering, Pukyong National University, Busan 48547, Republic of Korea.
  • Department of Chemical Engineering, Faculty of Industrial Engineering, Universitas Pembangunan Nasional "Veteran" Yogyakarta, Yogyakarta 55283, Indonesia.
  • Department of Polymer Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • BB21+ Project Team, Pukyong National University, Busan 48547, Republic of Korea.

ORCID-Profile: Yuli Nurul Maulida, Ellana Nabilah Nur Averina Ansar, PilHo Huh

Förderung

  • Ministry of Trade, Industry and Energy
  • Pukyong National University

Zitieren

APA

Maulida, Y. N., Ansar, E. N. N. A., Biutty, M. N., Huh, P., & Yoo, S. I. (2026). Mechanical Reinforcement and Early-Stage Deterioration of Cellulose Nanocrystal-Reinforced Isosorbide-Based Polycarbonate Nanocomposites Under Humid Soil Exposure. Polymers, 18(21), 2751. https://doi.org/10.3390/polym18212751

Vancouver

Maulida YN, Ansar ENNA, Biutty MN, Huh P, Yoo SI. Mechanical Reinforcement and Early-Stage Deterioration of Cellulose Nanocrystal-Reinforced Isosorbide-Based Polycarbonate Nanocomposites Under Humid Soil Exposure. Polymers. 2026;18(21):2751. doi:10.3390/polym18212751

BibTeX
@article{Maulida2026,
  author = {Maulida, Yuli Nurul and Ansar, Ellana Nabilah Nur Averina and Biutty, Merreta Noorenza and Huh, PilHo and Yoo, Seong Il},
  title = {Mechanical Reinforcement and Early-Stage Deterioration of Cellulose Nanocrystal-Reinforced Isosorbide-Based Polycarbonate Nanocomposites Under Humid Soil Exposure},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {21},
  pages = {2751},
  doi = {10.3390/polym18212751}
}
Kostenlos starten →