EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Influence of Self-Adhesive Resin Composite Deep Marginal Elevation on the Sealing Ability of CAD/CAM Lithium Disilicate Glass-Ceramic Inlays: An In Vitro Study

Rasha Haridy iD, Shadan Almotairi, Shoroug Alshehri, Abrar Nasser Bin Nooh iD, Moataz Elgezawi iD

Polymers · 22.06.2026 · 18 (12) · 1555

DOI: 10.3390/polym18121555 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 22.06.2026. Verfasst von Rasha Haridy und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Clinical Dental Sciences, College of Dentistry, Princess Nourah bint Abdulrahman University, P.O. Box 84428, Riyadh 11671, Saudi Arabia. Die Arbeit nennt 24 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Deep margin elevation (DME) is a conservative technique used to relocate subgingival proximal margins to a more favorable supragingival position, facilitating adhesive procedures and impression taking. This in vitro study evaluated the influence of two DME materials—a universal flowable resin composite and a self-adhesive flowable resin composite—on the cervical interfacial sealing ability of lithium disilicate glass–ceramic CAD/CAM inlay restorations. Twenty extracted maxillary premolars were randomly allocated into two groups (n = 10). Group A received DME using a universal flowable resin composite (3M™ Filtek™ Z350 XT) preceded by a conventional adhesive system, while Group B received DME using a self-adhesive flowable resin composite (Vertise™ Flow). All teeth were restored with lithium disilicate CAD/CAM inlays (CEREC Tessera) cemented with a self-adhesive resin cement (Breeze®). Specimens underwent thermocycling (10,000 cycles; 5–55 °C). Marginal gaps were assessed at the DME interface using high-resolution micro-computed tomography (micro-CT) in both coronal and sagittal cross-sections, before and after thermocycling. Statistically significant differences were found between groups in both sections before and after thermocycling (p < 0.05). The self-adhesive composite (Group B) demonstrated significantly lower gap values compared to the universal flowable composite (Group A) in both coronal and sagittal assessments. Thermocycling increased the gap in both groups; however, Group B maintained considerably lower leakage. The self-adhesive resin composite showed superior sealing ability at the DME interface compared to the universal flowable composite when used under lithium disilicate glass–ceramic inlay restorations. Further clinical studies are recommended to validate these findings.

Schlagwörter

Stichwörter der Autor:innen

CAD/CAMcervical margin relocationdeep margin elevationgapglass–ceramic inlaylithium disilicatemicro-CTself-adhesive resin composite

Autor:innen und Institutionen

  • Department of Clinical Dental Sciences, College of Dentistry, Princess Nourah bint Abdulrahman University, P.O. Box 84428, Riyadh 11671, Saudi Arabia.
  • Department of Conservative Dentistry, Faculty of Dentistry, Cairo University, Cairo 4240310, Egypt.
  • Internship Program, College of Dentistry, Princess Nourah bint Abdulrahman University, Riyadh 11671, Saudi Arabia.
  • Dental Clinics Department, King Abdullah bin Abdulaziz University Hospital, Princess Nourah bint Abdulrahman University, Riyadh 11671, Saudi Arabia.
  • Department of Restorative Dental Sciences, College of Dentistry, Imam Abdulrahman Bin Faisal University, P.O. Box 1982, Dammam 31441, Saudi Arabia.

ORCID-Profile: Rasha Haridy, Abrar Nasser Bin Nooh, Moataz Elgezawi

Zitieren

APA

Haridy, R., Almotairi, S., Alshehri, S., Nooh, A. N. B., & Elgezawi, M. (2026). Influence of Self-Adhesive Resin Composite Deep Marginal Elevation on the Sealing Ability of CAD/CAM Lithium Disilicate Glass-Ceramic Inlays: An In Vitro Study. Polymers, 18(12), 1555. https://doi.org/10.3390/polym18121555

Vancouver

Haridy R, Almotairi S, Alshehri S, Nooh ANB, Elgezawi M. Influence of Self-Adhesive Resin Composite Deep Marginal Elevation on the Sealing Ability of CAD/CAM Lithium Disilicate Glass-Ceramic Inlays: An In Vitro Study. Polymers. 2026;18(12):1555. doi:10.3390/polym18121555

BibTeX
@article{Haridy2026,
  author = {Haridy, Rasha and Almotairi, Shadan and Alshehri, Shoroug and Nooh, Abrar Nasser Bin and Elgezawi, Moataz},
  title = {Influence of Self-Adhesive Resin Composite Deep Marginal Elevation on the Sealing Ability of CAD/CAM Lithium Disilicate Glass-Ceramic Inlays: An In Vitro Study},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {12},
  pages = {1555},
  doi = {10.3390/polym18121555}
}
Kostenlos starten →