Fachartikel in der Zeitschrift Materials, online erschienen am 19.12.2023. Verfasst von Rana Turunç Oğuzman und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Dentistry, Altınbaş University, 34147 Istanbul, Turkey. Die Arbeit wurde bisher 13-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Ensuring optimum bond strength during cementation is vital for restoration success, with the practicality of the process being crucial in clinical practice. This study analyzed the effect of a single-step self-etching ceramic primer (MEP) and various surface treatments on the microshear bond strength (µSBS) between resin cement and glass-ceramic or polymer-based ceramic CAD/CAM materials. Specimens were fabricated from leucite-based glass-ceramic (LEU), lithium disilicate glass-ceramic (LDC), resin nanoceramic (RNC), and polymer infiltrated ceramic network (PICN) (n = 160). They were then classified based on the surface treatments (n = 10): control (no treatment); sandblasting with Al2O3 (AL); etching with hydrofluoric acid (HF); and MEP application. Scanning electron microscopy was used to evaluate the surface topography. µSBS was measured after cementation and thermocycling procedures. Failure modes were examined with a stereomicroscope. Statistical analysis involved two-way analysis of variance and Tukey HSD tests with a significance level of 0.05. µSBS was significantly influenced by both surface treatment and CAD/CAM material type. The most enhanced µSBS values for each material, regarding the surface treatment, were: LEU and LDC, HF; RNC, AL; PICN, AL or HF. MEP significantly increased the µSBS values of CAD/CAM materials except RNC, yet it did not yield the highest µSBS values for any of them.

Schlagwörter

Stichwörter der Autor:innen

10-MDPCAD/CAM materialsbond strengthself-etching ceramic primersurface treatments

Autor:innen und Institutionen

  • Department of Prosthodontics, Faculty of Dentistry, Altınbaş University, 34147 Istanbul, Turkey.
  • Department of Restorative Dentistry, Faculty of Dentistry, Istanbul University-Cerrahpaşa, 34098 Istanbul, Turkey.

ORCID-Profile: Rana Turunç Oğuzman, Soner Şişmanoğlu

Zitieren

APA

Turunç Oğuzman, R., & Şişmanoğlu, S. (2023). Adhesive Performance of Resin Cement to Glass-Ceramic and Polymer-Based Ceramic CAD/CAM Materials after Applying Self-Etching Ceramic Primer or Different Surface Treatments. Materials, 17(1), 2. https://doi.org/10.3390/ma17010002

Vancouver

Turunç Oğuzman R, Şişmanoğlu S. Adhesive Performance of Resin Cement to Glass-Ceramic and Polymer-Based Ceramic CAD/CAM Materials after Applying Self-Etching Ceramic Primer or Different Surface Treatments. Materials. 2023;17(1):2. doi:10.3390/ma17010002

BibTeX
@article{TurunOuzman2023,
  author = {Turunç Oğuzman, Rana and Şişmanoğlu, Soner},
  title = {Adhesive Performance of Resin Cement to Glass-Ceramic and Polymer-Based Ceramic CAD/CAM Materials after Applying Self-Etching Ceramic Primer or Different Surface Treatments},
  journal = {Materials},
  year = {2023},
  volume = {17},
  number = {1},
  pages = {2},
  doi = {10.3390/ma17010002}
}
Kostenlos starten →