Fachartikel in der Zeitschrift Polymers, online erschienen am 05.05.2026. Verfasst von Arun Biradar und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Mechanical Engineering, University of Alberta, 9211-116 St, Edmonton, AB T6G 1H9, Canada. Die Arbeit nennt 29 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Natural Sciences and Engineering Research Council of Canada.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Polyethylene of Raised Temperature resistance (PE-RT) is a versatile polymer with an enhanced ability to withstand higher temperatures than other standard polyethylene-derived materials. The application scope of PE-RT pipes extends across a broad range of residential and industrial uses. However, the inherent residual stresses developed during the fabrication processes of these pipes pose a significant challenge to their service performance. Moreover, the technical literature on residual stresses in PE-RT pipes is scarce. The investigations presented in this paper address this scientific and technical gap by experimentally quantifying the residual stresses present in different sizes of PE-RT pipes manufactured at the same plant. The slitting method was employed as the primary experimental procedure in these investigations. In addition to establishing experimental processes, this study aims to mitigate residual stresses in PE-RT pipes by investigating their sensitivity to varying annealing temperatures for one selected pipe size. Subsequently, the optimal annealing temperature (115 °C) was applied to the remaining pipe sizes to determine its efficacy in residual stress mitigation. Through the implementation of these procedures, the circumferential residual stresses in PE-RT pipes subjected to annealing at 115 °C were significantly reduced, with a minimum decrease of 78%. Furthermore, the longitudinal residual stresses were substantially diminished, reaching a state of near-complete elimination.

Schlagwörter

Stichwörter der Autor:innen

PE-RTannealingcrystallinitypolymer pipesresidual stress

Autor:innen und Institutionen

  • Department of Mechanical Engineering, University of Alberta, 9211-116 St, Edmonton, AB T6G 1H9, Canada.

ORCID-Profile: Arun Biradar, Pierre Mertiny

Förderung

  • Natural Sciences and Engineering Research Council of Canada

Zitieren

APA

Biradar, A., & Mertiny, P. (2026). Investigation of Residual Stresses in Extruded Thermoplastic PE-RT Pipes. Polymers, 18(9), 1135. https://doi.org/10.3390/polym18091135

Vancouver

Biradar A, Mertiny P. Investigation of Residual Stresses in Extruded Thermoplastic PE-RT Pipes. Polymers. 2026;18(9):1135. doi:10.3390/polym18091135

BibTeX
@article{Biradar2026,
  author = {Biradar, Arun and Mertiny, Pierre},
  title = {Investigation of Residual Stresses in Extruded Thermoplastic PE-RT Pipes},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {9},
  pages = {1135},
  doi = {10.3390/polym18091135}
}
Kostenlos starten →