EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Water Desorption Governs Glass Transition Recovery in Aligner Polymers

Luka Šimunović iD, Luka Brenko iD, Ana Marija Miličević, Tatjana Haramina iD, Senka Meštrović iD

Polymers · 21.04.2026 · 18 (8) · 1008

DOI: 10.3390/polym18081008 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 21.04.2026. Verfasst von Luka Šimunović und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Orthodontics, School of Dental Medicine, University of Zagreb, 10000 Zagreb, Croatia. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: University of Zagreb, European Union, National Recovery and Resilience Plan.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The clinical effectiveness of clear orthodontic aligners mainly depends on the thermomechanical stability of the polymers in this challenging hydrothermal environment. In this study, we compare the water-induced viscoelastic changes and glass transition temperature (Tg) stability of four polymers with different microarchitectures. Specifically, we examined directly printed photopolymer networks (Tera Harz TC-85 and LuxCreo 4D Aligner), a monolithic thermoplastic (Duran+), and a multilayer thermoplastic (ClearCorrect). Samples were immersed in physiological saline (0.9 wt.% NaCl) at 37 °C for 7 days, and Dynamic Mechanical Analysis (DMA) was performed in three conditions: dry, after immersion, and after a 2 h desorption step, mimicking a typical clinical 22:2 wear cycle. All polymers showed a decrease in Tg after immersion, with TC-85 exhibiting the greatest reduction relative to the dry baseline. Tg recovery after a 2 h ambient desorption step was incomplete and was significantly associated with the amount of water retained after 2 h drying (expressed as % of initial uptake; R2 = 0.419), whereas total water absorption after 7 days was not associated with short-term thermal recovery.

Schlagwörter

Stichwörter der Autor:innen

3D printingdynamic mechanical analysisglass transition temperaturehydroplasticizationmoisture desorptionorthodontic alignersphotopolymers

Autor:innen und Institutionen

  • Department of Orthodontics, School of Dental Medicine, University of Zagreb, 10000 Zagreb, Croatia.
  • Department of Materials, Faculty of Mechanical Engineering and Naval Architecture, University of Zagreb, 10000 Zagreb, Croatia.

ORCID-Profile: Luka Šimunović, Luka Brenko, Tatjana Haramina, Senka Meštrović

Förderung

  • University of Zagreb
  • European Union
  • National Recovery and Resilience Plan

Zitieren

APA

Šimunović, L., Brenko, L., Miličević, A. M., Haramina, T., & Meštrović, S. (2026). Water Desorption Governs Glass Transition Recovery in Aligner Polymers. Polymers, 18(8), 1008. https://doi.org/10.3390/polym18081008

Vancouver

Šimunović L, Brenko L, Miličević AM, Haramina T, Meštrović S. Water Desorption Governs Glass Transition Recovery in Aligner Polymers. Polymers. 2026;18(8):1008. doi:10.3390/polym18081008

BibTeX
@article{imunovi2026,
  author = {Šimunović, Luka and Brenko, Luka and Miličević, Ana Marija and Haramina, Tatjana and Meštrović, Senka},
  title = {Water Desorption Governs Glass Transition Recovery in Aligner Polymers},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {8},
  pages = {1008},
  doi = {10.3390/polym18081008}
}