Lifetime Prediction and Aging Characteristics of HTV-SiR Under Coupled Electro–Thermo–Hygro–Mechanical Stresses

Ben Shang iD, Wenjie Fu, Lei Yang, Qifan Yang iD, Zian Yuan, Zijiang Wang, Youping Fan iD

Polymers · 2026-04-14 · 18 (8) · 955

DOI: 10.3390/polym18080955 ↗

At a glance

Journal article in Polymers, published online on 2026-04-14. Written by Ben Shang and 6 co-authors. Institution: School of Electrical Engineering and Automation, Wuhan University, Wuhan 430072, China. Cited 1 times so far (Crossref); 28 references. The full text is freely available (open access, CC BY 4.0). Funded by: National Key Research and Development Program of China.

AbstractSubjectsBibliografiske oplysningerCiteRelated studies

Abstract (original language)

To investigate the aging behavior of high-temperature-vulcanized silicone rubber (HTV-SiR) used in composite insulator sheds under coupled electrical, thermal, humidity, and mechanical stresses, accelerated aging tests were conducted to emulate the service conditions of ±800 kV ultra-high-voltage direct current (UHVDC) systems in Guangzhou, China. The physicochemical, mechanical, and electrical properties of the specimens were systematically characterized. The results show simultaneous degradation of both electrical and mechanical performance. In particular, the tensile strength exhibits a significant monotonic decrease and drops to 49.52% of its initial value under the most severe condition (0.5 kV·mm−1 and 5% tensile strain) after 75 days. In contrast, the DC breakdown strength shows a non-monotonic “rise-then-fall” trend and decreases more markedly with increasing tensile strain. To address the one-shot and destructive nature of tensile testing and the associated statistical uncertainties, a lifetime prediction framework was developed by integrating a generalized Eyring acceleration relation with a stochastic degradation process. Under representative service conditions of 0.09 kV·mm−1 and 0.2% tensile strain, the predicted lifetimes corresponding to failure probabilities of 10%, 75%, and 90% are 1.77, 9.08, and 17.90 years, respectively. The applicability of the model is supported by field-aged specimens. These findings provide a mechanistically grounded and reliability-oriented basis for condition assessment, lifetime-margin evaluation, material screening, and maintenance planning of UHVDC composite insulators operating in hot–humid environments.

Subjects

Author keywords

composite insulatorgeneralized Eyring relationshiplifetime predictionpolymer degradationsilicone rubber

Authors and institutions

  • School of Electrical Engineering and Automation, Wuhan University, Wuhan 430072, China.
  • Institute of Next Generation Power Systems and International Standards, Wuhan University, Wuhan 430072, China.
  • China Electric Power Research Institute, Wuhan 430072, China.
  • School of Electrical Engineering, North China University of Water Resources and Electric Power, Wuhan 430072, China.

ORCID profiles: Ben Shang, Qifan Yang, Youping Fan

Funding

  • National Key Research and Development Program of China

Cite

APA

Shang, B., Fu, W., Yang, L., Yang, Q., Yuan, Z., Wang, Z., & Fan, Y. (2026). Lifetime Prediction and Aging Characteristics of HTV-SiR Under Coupled Electro–Thermo–Hygro–Mechanical Stresses. Polymers, 18(8), 955. https://doi.org/10.3390/polym18080955

Vancouver

Shang B, Fu W, Yang L, Yang Q, Yuan Z, Wang Z, et al. Lifetime Prediction and Aging Characteristics of HTV-SiR Under Coupled Electro–Thermo–Hygro–Mechanical Stresses. Polymers. 2026;18(8):955. doi:10.3390/polym18080955

BibTeX
@article{Shang2026,
  author = {Shang, Ben and Fu, Wenjie and Yang, Lei and Yang, Qifan and Yuan, Zian and Wang, Zijiang and Fan, Youping},
  title = {Lifetime Prediction and Aging Characteristics of HTV-SiR Under Coupled Electro–Thermo–Hygro–Mechanical Stresses},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {8},
  pages = {955},
  doi = {10.3390/polym18080955}
}
Start for free →