Fachartikel in der Zeitschrift Polymers, online erschienen am 10.07.2024. Verfasst von Kartik Behera und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Chemical and Materials Engineering, Chang Gung University, Taoyuan 333, Taiwan. Die Arbeit wurde bisher 18-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Chang Gung Memorial Hospital (Taoyuan, Taiwan):, National Science and Technology Council (NSTC, Taiwan), Chang Gung Memorial Hospital.
Abstract (Originalsprache)
In this study, a twin-screw extruder was used to fabricate poly(lactic acid) (PLA)/poly(butylene adipate-co-terephthalate) (PBAT) blends and blend-based nanocomposites with carbon nanotube (CNT) or nanocarbon black (CB) as nanofillers. The fabricated samples were subsequently treated with supercritical carbon dioxide (scCO2) to fabricate the corresponding foams. Bi-phasic morphology and selective distribution of CNTs or CBs in the PBAT phase were observed in the blends/composites through scanning electron microscopy. After the scCO2 treatment, the selective foaming of the PBAT phase in the prepared blends/composites was confirmed. The cellular structure of PBAT phase in scCO2-treated blends is similar to the size/shape of PBAT domains in untreated blends or treated neat PBAT foam. The addition of CNTs or CBs in the blends led to a slight reduction in cell size of the foamed PBAT phase, demonstrating CNT/CB-induced cell nucleation. Differential scanning calorimetry (DSC) results showed that CNTs and CBs played as nucleating agents and increased the initial crystallization temperature up to 14 °C compared with neat PBAT for PBAT in different composites during cooling. The scCO2 treatment induced the bimodal stability of PBAT crystals in different samples, which melted mainly in two temperature regions in DSC studies. Thermogravimetric analyses revealed that compared with parent blends, the addition of CNTs or CBs increased the temperature at 80 wt.% loss (degradation of PBAT portion) up to 6 °C. The electrical resistivity decreased by more than six orders of magnitude for certain CNT- or CB-added composites compared with the parent blends. The hardness of the blends slightly increased after forming the corresponding composites and then declined after the scCO2 treatment.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Chemical and Materials Engineering, Chang Gung University, Taoyuan 333, Taiwan.
- Department of General Dentistry, Chang Gung Memorial Hospital, Taoyuan 333, Taiwan.
- Department of Chemical Engineering, Ming Chi University of Technology, New Taipei City 243, Taiwan.
Förderung
- Chang Gung Memorial Hospital (Taoyuan, Taiwan):
- National Science and Technology Council (NSTC, Taiwan)
- Chang Gung Memorial Hospital
Zitieren
APA
Behera, K., Tsai, C. H., Liao, X. B., & Chiu, F. C. (2024). Fabrication and Characterization of PLA/PBAT Blends, Blend-Based Nanocomposites, and Their Supercritical Carbon Dioxide-Induced Foams. Polymers, 16(14), 1971. https://doi.org/10.3390/polym16141971
Vancouver
Behera K, Tsai CH, Liao XB, Chiu FC. Fabrication and Characterization of PLA/PBAT Blends, Blend-Based Nanocomposites, and Their Supercritical Carbon Dioxide-Induced Foams. Polymers. 2024;16(14):1971. doi:10.3390/polym16141971
BibTeX
@article{Behera2024,
author = {Behera, Kartik and Tsai, Chien-Hsing and Liao, Xiang-Bo and Chiu, Fang-Chyou},
title = {Fabrication and Characterization of PLA/PBAT Blends, Blend-Based Nanocomposites, and Their Supercritical Carbon Dioxide-Induced Foams},
journal = {Polymers},
year = {2024},
volume = {16},
number = {14},
pages = {1971},
doi = {10.3390/polym16141971}
}
EUVIMED