Fachartikel in der Zeitschrift Polymers, online erschienen am 08.07.2024. Verfasst von Saifeng Tang und 6 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Alternate Electrical Power System with Renewable Energy Sources, North China Electric Power University, Beijing 102206, China. Die Arbeit wurde bisher 37-mal zitiert (Crossref) und nennt 44 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the Fundamental Research Funds for the Central Universities, Fundamental Research Funds for the Central Universities.
Abstract (Originalsprache)
Natural rubber (NR) composites have been widely applied in damping products to reduce harmful vibrations, while rubber with only a single composition barely meets performance requirements. In this study, rubber blend composites including various ratios of NR and styrene butadiene rubber (SBR) were prepared via the conventional mechanical blending method. The effects of the rubber components on the compression set, compression fatigue temperature rising and the thermal oxidative aging properties of the NR/SBR blend composites were investigated. Meanwhile, the dynamic mechanical thermal analyzer and rubber processing analyzer were used to characterize the dynamic viscoelasticity of the NR/SBR blend composites. It was shown that, with the increase in the SBR ratio, the vulcanization rate of the composites increased significantly, while the compression fatigue temperature rising of the composites decreased gradually from 47 °C (0% SBR ratio) to 31 °C (50% SBR ratio). The compression set of the composites remained at ~33% when the SBR ratio was no more than 20%, and increased gradually when the SBR ratio was more than 20%.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Alternate Electrical Power System with Renewable Energy Sources, North China Electric Power University, Beijing 102206, China.
- South China Institute of Environmental Sciences, Ministry of Ecology and Environment, Guangzhou 510655, China.
ORCID-Profile: Saifeng Tang, Jian Wang
Förderung
- the Fundamental Research Funds for the Central Universities
- Fundamental Research Funds for the Central Universities
Zitieren
APA
Tang, S., Li, Z., Sun, W., Liu, Y., Wang, J., Wang, X., & Lin, J. (2024). Natural Rubber/Styrene–Butadiene Rubber Blend Composites Potentially Applied in Damping Bearings. Polymers, 16(13), 1945. https://doi.org/10.3390/polym16131945
Vancouver
Tang S, Li Z, Sun W, Liu Y, Wang J, Wang X, et al. Natural Rubber/Styrene–Butadiene Rubber Blend Composites Potentially Applied in Damping Bearings. Polymers. 2024;16(13):1945. doi:10.3390/polym16131945
BibTeX
@article{Tang2024,
author = {Tang, Saifeng and Li, Zhanxu and Sun, Weichong and Liu, Yangling and Wang, Jian and Wang, Xiong and Lin, Jun},
title = {Natural Rubber/Styrene–Butadiene Rubber Blend Composites Potentially Applied in Damping Bearings},
journal = {Polymers},
year = {2024},
volume = {16},
number = {13},
pages = {1945},
doi = {10.3390/polym16131945}
}
EUVIMED