Effect of Inorganic Fillers on Electrical and Mechanical Properties of Ceramizable Silicone Rubber
Polymers · 14.06.2024 · 16 (12) · 1695
DOI: 10.3390/polym16121695 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymers, online erschienen am 14.06.2024. Verfasst von Mingyuan Yang und 8 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Power Transmission Equipment Technology, School of Electrical Engineering, Chongqing University, Chongqing 400044, China. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 67 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Fok Ying-Tong Education Foundation, Fund of the National Natural Science Foundation of China.
Abstract (Originalsprache)
Ceramizable silicone rubber (CSR) composed of silicone rubber matrix and inorganic fillers can be transformed into a dense flame-retardant ceramic upon encountering high temperatures or flames. Conventionally, CSR can be sintered into a dense ceramic at temperatures above 1000 °C, which is higher than the melting point of a copper conductor used in a power cable. In this study, the vulcanization process and mass ratio of inorganic fillers of CSR were studied to lower its ceramization temperature to 950 °C. The electrical and mechanical properties of CSRs and their ceramic bulks were studied with various ratios of wollastonite and muscovite. It was found that the CSR samples could be successfully fabricated using a two-step vulcanization technique (at 120 °C and 150 °C, respectively). As a high ratio of muscovite filler was introduced into the CSR, the sample presented a high dc electrical resistivity of 6.713 × 1014 Ω·cm, and a low dielectric constant of 4.3 and dielectric loss of 0.025 at 50 Hz. After the thermal sintering (at 950 °C for 1 h) of the CSR sample with a high ratio of muscovite, the ceramic sample exhibits a dense microstructure without any pores. The ceramic also demonstrates excellent insulating properties, with a volume resistivity of 8.69 × 1011 Ω·cm, and a low dielectric loss of 0.01 at 50 Hz. Meanwhile, the three-point bending strength of the ceramic sample reaches a value of 110.03 MPa. This study provides a potential route to fabricate CSR used for fire-resistant cables.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Power Transmission Equipment Technology, School of Electrical Engineering, Chongqing University, Chongqing 400044, China.
- Faculty of Electrical and Control Engineering, Liaoning Technical University, Fuxin 123032, China.
- State Grid Chongqing Electric Power Research Institute, Chongqing 401121, China.
ORCID-Profile: Xuetong Zhao
Förderung
- National Natural Science Foundation of China
- Fok Ying-Tong Education Foundation
- Fund of the National Natural Science Foundation of China
Zitieren
APA
Yang, M., Qiao, J., Su, B., Xiao, Y., Kang, S., Li, Y., Cao, H., Tang, H., & Zhao, X. (2024). Effect of Inorganic Fillers on Electrical and Mechanical Properties of Ceramizable Silicone Rubber. Polymers, 16(12), 1695. https://doi.org/10.3390/polym16121695
Vancouver
Yang M, Qiao J, Su B, Xiao Y, Kang S, Li Y, et al. Effect of Inorganic Fillers on Electrical and Mechanical Properties of Ceramizable Silicone Rubber. Polymers. 2024;16(12):1695. doi:10.3390/polym16121695
BibTeX
@article{Yang2024,
author = {Yang, Mingyuan and Qiao, Jingqi and Su, Bolin and Xiao, Yongjian and Kang, Shenglin and Li, Yuchen and Cao, Hanzhong and Tang, Hongchuan and Zhao, Xuetong},
title = {Effect of Inorganic Fillers on Electrical and Mechanical Properties of Ceramizable Silicone Rubber},
journal = {Polymers},
year = {2024},
volume = {16},
number = {12},
pages = {1695},
doi = {10.3390/polym16121695}
}
EUVIMED