Residual Stress and Warping Analysis of the Nano-Silver Pressureless Sintering Process in SiC Power Device Packaging

Wenchao Tian, Dexin Li, Haojie Dang iD, Shiqian Liang, Yizheng Zhang, Xiaojun Zhang, Si Chen, Xiaochuan Yu

Micromachines · 28.08.2024 · 15 (9) · 1087

DOI: 10.3390/mi15091087 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Micromachines, online erschienen am 28.08.2024. Verfasst von Wenchao Tian und 7 weiteren Autor:innen. Beteiligte Einrichtung: School of Electro-Mechanical Engineering, Xidian University, Xi'an 710071, China. Die Arbeit wurde bisher 15-mal zitiert (Crossref) und nennt 29 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Stabilization Support Fund.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Chip bonding, an essential process in power semiconductor device packaging, commonly includes welding and nano-silver sintering. Currently, most of the research on chip bonding technology focuses on the thermal stress analysis of tin–lead solder and nano-silver pressure-assisted sintering, whereas research on the thermal stress analysis of the nano-silver pressureless sintering process is more limited. In this study, the pressureless sintering process of nano-silver was studied using finite element software, with nano-silver as an interconnect material. Using the control variable method, we analyzed the influences of sintering temperature, cooling rate, solder paste thickness, and solder paste area on the residual stress and warping deformation of power devices. In addition, orthogonal experiments were designed to optimize the parameters and determine the optimal combination of the process parameters. The results showed that the maximum residual stress of the module appeared on the connection surface between the power chip and the nano-silver solder paste layer. The module warping deformation was convex warping. The residual stress of the solder layer increased with the increase in sintering temperature and cooling rate. It decreased with the increase in coating thickness. With the increase in the coating area, it showed a wave change. Each parameter influenced the stress of the solder layer in this descending order: sintering temperature, cooling rate, solder paste area, and solder paste thickness. The residual stress of the nano-silver layer was 24.83 MPa under the optimal combination of the process parameters and was reduced by 29.38% compared with the original value of 35.162 MPa.

Schlagwörter

Stichwörter der Autor:innen

SiCnano-silver pastepressureless sinteringresidual stresswarpage

Autor:innen und Institutionen

  • School of Electro-Mechanical Engineering, Xidian University, Xi'an 710071, China.
  • State Key Laboratory of Electromechanical Integrated Manufacturing of High-Performance Electronic Equipments, Xi'an 710071, China.
  • The Thirteenth Research Institute of China Electronics Group Corporation, Shijiazhuang 050000, China.
  • The Fifth Electronics Research Institute of Ministry of Industry and Information Technology, Guangzhou 510000, China.
  • Shandong Junyu Electronic Technology Co., Ltd., Linyi 276100, China.

ORCID-Profile: Haojie Dang

Förderung

  • Stabilization Support Fund

Zitieren

APA

Tian, W., Li, D., Dang, H., Liang, S., Zhang, Y., Zhang, X., Chen, S., & Yu, X. (2024). Residual Stress and Warping Analysis of the Nano-Silver Pressureless Sintering Process in SiC Power Device Packaging. Micromachines, 15(9), 1087. https://doi.org/10.3390/mi15091087

Vancouver

Tian W, Li D, Dang H, Liang S, Zhang Y, Zhang X, et al. Residual Stress and Warping Analysis of the Nano-Silver Pressureless Sintering Process in SiC Power Device Packaging. Micromachines. 2024;15(9):1087. doi:10.3390/mi15091087

BibTeX
@article{Tian2024,
  author = {Tian, Wenchao and Li, Dexin and Dang, Haojie and Liang, Shiqian and Zhang, Yizheng and Zhang, Xiaojun and Chen, Si and Yu, Xiaochuan},
  title = {Residual Stress and Warping Analysis of the Nano-Silver Pressureless Sintering Process in SiC Power Device Packaging},
  journal = {Micromachines},
  year = {2024},
  volume = {15},
  number = {9},
  pages = {1087},
  doi = {10.3390/mi15091087}
}