EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of Deep Cryogenic Aging Treatment on Microstructure and Mechanical Properties of Selective Laser-Melted AlSi10Mg Alloy

Pengjun Tang, Taiqi Yan, Yu Wu, Haibo Tang

Metals · 24.04.2024 · 14 (5) · 493

DOI: 10.3390/met14050493 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 24.04.2024. Verfasst von Pengjun Tang und 3 weiteren Autor:innen. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Aero Engine Corporation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Deep cryogenic aging (DCA) is a newly developed heat treatment technique for additive-manufactured metallic materials to reduce residual stress and improve their mechanical properties. In this study, AlSi10Mg alloy samples fabricated by selective laser melting were deep-cryogenic-treated at −160 °C and subsequently aged at 160 °C. Phase and microstructural analyses were conducted using X-ray diffraction, optical microscopy, scanning electron microscopy, and transmission electron microscopy, while the mechanical properties were evaluated through microhardness and tensile testing at room temperature. The results indicated that the DCA treatment did not have an effect on the morphology of the melt pools. However, it facilitated the formation of atomic clusters and nanoscale Si and β′ phases, as well as accelerating the coarsening of grains and the ripening of the eutectic Si phase. After DCA treatment, the mass fraction of the Si phase experienced an increase from 4.4% to 7.2%. Concurrently, the volume fraction of the precipitated secondary phases elevated to 5.1%. The microhardness was enhanced to 147 HV, and the ultimate tensile strength and yield strength achieved 495 MPa and 345 MPa, respectively, with an elongation of 7.5%. In comparison to the as-built specimen, the microhardness, ultimate tensile strength, and yield strength increased by 11.4%, 3.1%, and 19.0%, respectively. The improvement in mechanical properties is primarily attributed to the Orowan strengthening mechanism induced by the secondary phases.

Förderung

  • National Natural Science Foundation of China
  • Aero Engine Corporation of China

Zitieren

APA

Tang, P., Yan, T., Wu, Y., & Tang, H. (2024). Effect of Deep Cryogenic Aging Treatment on Microstructure and Mechanical Properties of Selective Laser-Melted AlSi10Mg Alloy. Metals, 14(5), 493. https://doi.org/10.3390/met14050493

Vancouver

Tang P, Yan T, Wu Y, Tang H. Effect of Deep Cryogenic Aging Treatment on Microstructure and Mechanical Properties of Selective Laser-Melted AlSi10Mg Alloy. Metals. 2024;14(5):493. doi:10.3390/met14050493

BibTeX
@article{Tang2024,
  author = {Tang, Pengjun and Yan, Taiqi and Wu, Yu and Tang, Haibo},
  title = {Effect of Deep Cryogenic Aging Treatment on Microstructure and Mechanical Properties of Selective Laser-Melted AlSi10Mg Alloy},
  journal = {Metals},
  year = {2024},
  volume = {14},
  number = {5},
  pages = {493},
  doi = {10.3390/met14050493}
}