Reduction Kinetics of Compact Hematite with Hydrogen from 600 to 1050 °C
Metals · 23.02.2023 · 13 (3) · 464
DOI: 10.3390/met13030464 ↗Kurz gefasst
Fachartikel in der Zeitschrift Metals, online erschienen am 23.02.2023. Verfasst von Junguo He und 3 weiteren Autor:innen. Die Arbeit wurde bisher 34-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the University of Science and Technology Beijing, China.
Abstract (Originalsprache)
Reduction of iron ores with hydrogen is a solution to replace fossil fuels. For this reason, it is important to discuss previous discrepancies. Some previous studies suggest a rate minimum with respect to temperature. Our research work indicates that a rate minimum can be avoided. Thermogravimetric isothermal reduction experiments were carried out from 600 to 1050 °C with pure reagent ferric oxide and hydrogen using a tubular furnace. The morphology and chemical composition of the initial sample, consisting of particulate hematite (Fe2O3), and the final product, consisting of metallic iron (Fe°), was defined using scanning electron microscopy (SEM) and X-ray diffraction (XRD). The reduction rate for the conversion from hematite to magnetite (Fe2O3 to Fe3O4) was the highest, around 5 %/min, decreasing to around 2–5%/min for the second stage of conversion from magnetite to wüstite (Fe3O4 to FeO). This reduction rate remains almost constant from about 20–80% reduction, decreasing to 0.3–1%/min for the completion of reduction from wüstite to metallic iron (FeO to Fe°). The reduction controlling mechanism was evaluated based on the calculated apparent activation energy and fitting the experimental data to one gas-solid reaction equation. Under the experimental conditions in this work, the reduction rate of pure hematite with hydrogen linearly increased with temperatures from 600 to 1000 °C, without a rate minimum in this temperature range. Above 1000 °C, the reduction rate decreased due to sintering phenomena. This result suggests a maximum reduction temperature of 1000 °C using pure hematite and hydrogen as the reducing gas. The reduction controlling mechanisms identified using hydrogen as a reducing gas were chemical reaction for the conversion from hematite to wüstite and diffusion control for the final reduction from wüstite to metallic iron. Since the reduction rate from wüstite to metallic iron is the one that affects the overall rate of reduction, overall changes in porosity were also evaluated. Finally, the reduction of wüstite is schematically described.
Förderung
- the University of Science and Technology Beijing, China
Zitieren
APA
He, J., Li, K., Zhang, J., & Conejo, A. N. (2023). Reduction Kinetics of Compact Hematite with Hydrogen from 600 to 1050 °C. Metals, 13(3), 464. https://doi.org/10.3390/met13030464
Vancouver
He J, Li K, Zhang J, Conejo AN. Reduction Kinetics of Compact Hematite with Hydrogen from 600 to 1050 °C. Metals. 2023;13(3):464. doi:10.3390/met13030464
BibTeX
@article{He2023,
author = {He, Junguo and Li, Kejiang and Zhang, Jianliang and Conejo, Alberto N.},
title = {Reduction Kinetics of Compact Hematite with Hydrogen from 600 to 1050 °C},
journal = {Metals},
year = {2023},
volume = {13},
number = {3},
pages = {464},
doi = {10.3390/met13030464}
}
EUVIMED