Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants

Vasilis Nikitakos iD, Athanasios D Porfyris iD, Triantafyllia Alevizaki, Eleni Rakanta, Beatriz Yecora, Angelica Perez, Rudolf Pfaendner iD, Constantine D Papaspyrides iD, Konstantinos G Beltsios

Materials · 09.11.2026 · 19 (21) · 4751

DOI: 10.3390/ma19214751 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 09.11.2026. Verfasst von Vasilis Nikitakos und 8 weiteren Autor:innen. Beteiligte Einrichtung: Laboratory of Polymer Technology, School of Chemical Engineering, National Technical University of Athens, 15780 Athens, Greece. Die Arbeit nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: European Health and Digital Executive Agency, European Union’s Horizon 2020 Research and Innovation Programme.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Poly(vinyl butyral) (PVB) is widely used as an interlayer in laminated safety glass in automotive and construction applications. The increasing quantities of PVB arising from end-of-life laminated glass represent a waste stream with significant potential for recycling. This study investigates the durability of high-quality retrieved PVB (re-PVB) separated from laminated glass wastes and evaluates the effect of restabilization against UV aging. Neat unplasticized PVB (u-PVB) and re-PVB were subjected to artificial UV weathering (ISO 4892-3) for up to 1500 h and then characterized in terms of chemical structure, yellowness, melt flow behavior and molecular weight. The results showed that u-PVB exhibited pronounced photooxidative degradation, while re-PVB remained comparatively stable. UV–Vis spectroscopy revealed the presence of residual UV absorbers in re-PVB, indicating that the components of the initial stabilization system might remain functional after the end of its life. Unexpectedly, the restabilization of re-PVB with phenolic antioxidants (AOs) reduced its photooxidative stability, despite their established effectiveness against thermo-mechanical degradation in melt reprocessing. A possible antagonistic effect was suggested between the newly introduced AOs and the residual stabilization system. These findings highlight that re-PVB is a valuable waste, and restabilization should be carefully considered when designing its second service life.

Schlagwörter

Stichwörter der Autor:innen

PVBinterlayerrecyclingstabilizersweathering

Autor:innen und Institutionen

  • Laboratory of Polymer Technology, School of Chemical Engineering, National Technical University of Athens, 15780 Athens, Greece.
  • Research Lab of Advanced, Composites, Nanomaterials and Nanotechnology (R-NanoLab), School of Chemical Engineering, National Technical University of Athens, 15780 Athens, Greece.
  • Department of Materials Science & Engineering, School of Chemical Engineering, Zographou Campus, National Technical University of Athens, 15780 Athens, Greece.
  • LUREDERRA Technological Centre, Perguita Industrial Area, 31210 Los Arcos, Spain.
  • Fraunhofer Institute for Structural Durability and System Reliability LBF, 64289 Darmstadt, Germany.

ORCID-Profile: Vasilis Nikitakos, Athanasios D Porfyris, Rudolf Pfaendner, Constantine D Papaspyrides

Förderung

  • European Health and Digital Executive Agency
  • European Union’s Horizon 2020 Research and Innovation Programme

Zitieren

APA

Nikitakos, V., Porfyris, A. D., Alevizaki, T., Rakanta, E., Yecora, B., Perez, A., Pfaendner, R., Papaspyrides, C. D., & Beltsios, K. G. (2026). Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants. Materials, 19(21), 4751. https://doi.org/10.3390/ma19214751

Vancouver

Nikitakos V, Porfyris AD, Alevizaki T, Rakanta E, Yecora B, Perez A, et al. Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants. Materials. 2026;19(21):4751. doi:10.3390/ma19214751

BibTeX
@article{Nikitakos2026,
  author = {Nikitakos, Vasilis and Porfyris, Athanasios D and Alevizaki, Triantafyllia and Rakanta, Eleni and Yecora, Beatriz and Perez, Angelica and Pfaendner, Rudolf and Papaspyrides, Constantine D and Beltsios, Konstantinos G},
  title = {Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {21},
  pages = {4751},
  doi = {10.3390/ma19214751}
}
Kostenlos starten →