EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effects of Packaging-Relevant Contaminants on the Property Evolution and Reprocessability of PET During Repeated Mechanical Recycling

Roderik Plavec, Slávka Hlaváčiková, Jozef Feranc iD, Henrieta Suchánková, Zuzana Kramárová, Michal Ďurfina iD, Leona Omaníková, Mohammadhassan Rahnama Hezaveh iD, Mária Straková, Nafiseh Babaei, Ján Kruželák iD, Tibor Dubaj iD und 1 weitere

Materials · 05.11.2026 · 19 (21) · 4704

DOI: 10.3390/ma19214704 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 05.11.2026. Verfasst von Roderik Plavec und 12 weiteren Autor:innen. Beteiligte Einrichtung: Institute of Natural and Synthetic Polymers, Faculty of Chemical and Food Technology, Slovak University of Technology, Radlinského 9, 812 37 Bratisla…. Die Arbeit nennt 78 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Vedecká grantová agentúra MŠVVaM SR a SAV (VEGA), Slovak Republic and the Slovak Academy of Sciences.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Residual polymeric contaminants from labels, closures, and adhesives can affect the quality and reprocessability of mechanically recycled polyethylene terephthalate (PET). Direct comparison of individual contaminants, however, is often complicated by differences in PET feedstock, contaminant concentration, and processing conditions among published studies. In this work, eight packaging-relevant contaminants—polypropylene (PP), low-density polyethylene (LDPE), high-density polyethylene (HDPE), polystyrene (PS), glycol-modified PET (PETG), poly(lactic acid) (PLA), poly(vinyl chloride) (PVC), and a commercial hot-melt labeling adhesive (HMA)—were compared at a fixed model concentration of 3 wt.% in bottle-grade PET under identical thermomechanical processing conditions. Contaminant selection was supported by ATR-FTIR screening of commercial bottle labels. Melt flow rate, MFR-derived intrinsic viscosity, differential scanning calorimetry, tensile properties, and CIE L*a*b* color characteristics were evaluated over successive processing stages. PET/PP, PET/LDPE, PET/HDPE, PET/PS, and PET/PETG remained processable through three processing stages, whereas PET/PLA and PET/HMA could only be processed through the second stage, and PET/PVC lost stable strand-forming ability after initial compounding. Tg and Tm remained comparatively stable, while crystallization temperature and PET crystallinity showed contaminant- and processing-dependent changes. Elongation at break was generally more sensitive to contamination than tensile strength, and PVC produced the most pronounced discoloration. Industrial PET fractions collected at successive separation and washing/decontamination stages were evaluated as a complementary case study. Progressive purification was associated with improved MFR-derived IV, while TGA showed only minor differences among the fractions. The results demonstrate that contaminant identity strongly affects PET property evolution and reprocessability during repeated mechanical recycling.

Schlagwörter

Stichwörter der Autor:innen

mechanical recyclingpolyethylene terephthalate (PET)polymer contaminationrepeated thermomechanical processing

Autor:innen und Institutionen

  • Institute of Natural and Synthetic Polymers, Faculty of Chemical and Food Technology, Slovak University of Technology, Radlinského 9, 812 37 Bratislava, Slovakia.
  • Institute of Physical Chemistry and Chemical Physics, Faculty of Chemical and Food Technology, Slovak University of Technology, Radlinského 9, 812 37 Bratislava, Slovakia.

ORCID-Profile: Jozef Feranc, Michal Ďurfina, Mohammadhassan Rahnama Hezaveh, Ján Kruželák, Tibor Dubaj, Pavol Alexy

Förderung

  • Vedecká grantová agentúra MŠVVaM SR a SAV (VEGA)
  • Slovak Republic and the Slovak Academy of Sciences

Zitieren

APA

Plavec, R., Hlaváčiková, S., Feranc, J., Suchánková, H., Kramárová, Z., Ďurfina, M., Omaníková, L., Hezaveh, M. R., Straková, M., Babaei, N., Kruželák, J., Dubaj, T., & Alexy, P. (2026). Effects of Packaging-Relevant Contaminants on the Property Evolution and Reprocessability of PET During Repeated Mechanical Recycling. Materials, 19(21), 4704. https://doi.org/10.3390/ma19214704

Vancouver

Plavec R, Hlaváčiková S, Feranc J, Suchánková H, Kramárová Z, Ďurfina M, et al. Effects of Packaging-Relevant Contaminants on the Property Evolution and Reprocessability of PET During Repeated Mechanical Recycling. Materials. 2026;19(21):4704. doi:10.3390/ma19214704

BibTeX
@article{Plavec2026,
  author = {Plavec, Roderik and Hlaváčiková, Slávka and Feranc, Jozef and Suchánková, Henrieta and Kramárová, Zuzana and Ďurfina, Michal and Omaníková, Leona and Hezaveh, Mohammadhassan Rahnama and Straková, Mária and Babaei, Nafiseh and Kruželák, Ján and Dubaj, Tibor and Alexy, Pavol},
  title = {Effects of Packaging-Relevant Contaminants on the Property Evolution and Reprocessability of PET During Repeated Mechanical Recycling},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {21},
  pages = {4704},
  doi = {10.3390/ma19214704}
}
Kostenlos starten →