Profilometric Quantification of Wear-Track Degradation in FFF Kevlar-Reinforced ASA Composites
Materials · 19.05.2026 · 19 (10) · 2135
DOI: 10.3390/ma19102135 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 19.05.2026. Verfasst von Patricia Isabela Brăileanu und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Robotics and Manufacturing Systems, Faculty of Industrial Engineering and Robotics, National University of Science and Technology POLIT…. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Fused filament fabrication (FFF) produces components with characteristic topographical features that influence their tribological behavior. Because conventional roughness parameters may not fully describe the localized surface degradation of reinforced FFF polymers, this study evaluates the wear-track evolution of FFF aramid fiber-reinforced Acrylonitrile Styrene Acrylate (ASA) composites using a comparative profilometric framework based on pre-wear and post-wear measurements. Specimens with different infill configurations underwent dry sliding Ball-on-Disc tribological testing, followed by profilometric wear-track analysis and optical microscopy inspection. The macroscopic wear response exhibited a non-monotonic dependence on infill configuration. Under the present experimental conditions, the 30% infill configuration showed the most favorable average wear response, with the lowest wear volume and specific wear rate, whereas the 90% infill configuration showed the highest material loss. To compare the surface modifications induced by sliding, three derived relative profilometric descriptors were evaluated: Surface Texture Alteration Index (STAI), Peak Deformation Index (PDI) and Material Ratio Preservation Index (MRPI). These descriptors were used as complementary comparative parameters rather than replacements for standardized roughness or Abbott–Firestone-based measurements. Statistical analysis showed a very strong association between maximum wear-track depth and calculated volumetric material loss, indicating that deeper wear-track profiles were consistently associated with higher material removal within the investigated dataset. Furthermore, correlation analysis suggested that the initial material ratio may be more closely associated with the subsequent wear response than the initial arithmetic mean roughness. This study indicates that combining wear volume, wear-track geometry, optical microscopy and relative profilometric descriptors provides a useful comparative approach for evaluating degradation in FFF Kevlar-reinforced ASA components under sliding conditions.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Robotics and Manufacturing Systems, Faculty of Industrial Engineering and Robotics, National University of Science and Technology POLITEHNICA BUCHAREST, RO-060042 Bucharest, Romania.
- National Institute for Laser, Plasma and Radiation Physics, RO-077125 Măgurele, Romania.
- Doctoral School of Industrial Engineering and Robotics, National University of Science and Technology POLITEHNICA BUCHAREST, RO-060042 Bucharest, Romania.
ORCID-Profile: Patricia Isabela Brăileanu, Marius-Teodor Mocanu
Zitieren
APA
Brăileanu, P. I., Mocanu, M. T., & Pascu, N. E. (2026). Profilometric Quantification of Wear-Track Degradation in FFF Kevlar-Reinforced ASA Composites. Materials, 19(10), 2135. https://doi.org/10.3390/ma19102135
Vancouver
Brăileanu PI, Mocanu MT, Pascu NE. Profilometric Quantification of Wear-Track Degradation in FFF Kevlar-Reinforced ASA Composites. Materials. 2026;19(10):2135. doi:10.3390/ma19102135
BibTeX
@article{Brileanu2026,
author = {Brăileanu, Patricia Isabela and Mocanu, Marius-Teodor and Pascu, Nicoleta Elisabeta},
title = {Profilometric Quantification of Wear-Track Degradation in FFF Kevlar-Reinforced ASA Composites},
journal = {Materials},
year = {2026},
volume = {19},
number = {10},
pages = {2135},
doi = {10.3390/ma19102135}
}
EUVIMED