EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Physical and Thermomechanical Performance of Kevlar and Carbon–Kevlar‐Reinforced Geopolymer Composites at Elevated Temperatures

Arup Kumar Debnath, Md. Abdul Hasib, Rizuanul Arefin Emon, Abdullah Al Kafi, Tanvir Ahmed Fahim, Md. Sanaul Rabbi

Journal of Engineering · 2025-01 · 2025 (1)

DOI: 10.1155/je/2424227 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Engineering, online erschienen am 30.10.2025. Verfasst von Arup Kumar Debnath und 5 weiteren Autor:innen. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 49 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Fiber‐reinforced geopolymer composites (GPCs) are garnering heightened interest owing to their exceptional thermal stability and mechanical properties relative to traditional cement‐based systems. Kevlar and carbon–Kevlar hybrids are notably advantageous due to their exceptional tensile strength, low density, and ability to maintain structural integrity at extreme temperatures. This study examines the mechanical and physical properties of GPCs reinforced with Kevlar fiber (KF) and hybrid carbon–Kevlar fiber (CKF) under elevated temperatures. Geopolymers are typically brittle at high temperatures, but fiber reinforcement enhances their thermal and mechanical resilience. Samples with 1%, 1.5%, and 2% fiber content were heated to 200°C, 400°C, 600°C, and 800°C. Mechanical properties such as compressive and flexural strength, along with physical properties like color, cracks, and voids, were evaluated, and thermal conductivity was measured. For KF‐reinforced composites (KF‐GPCs), the highest compressive (14.6 MPa) and flexural strengths (10.02 MPa) were observed at 200°C with 1% fiber content. Strength decreased as the fiber content increased and temperatures rose, with partial recovery at 800°C, presumably owing to microstructural densification and phase transitions that briefly improved load‐bearing capability, although ductility remained markedly diminished. In CKF‐reinforced composites (CKF‐GPCs), compressive and flexural strength increased with fiber content, peaking at 200°C with 2% fiber (10.86 MPa). However, CKF‐GPCs showed increased brittleness and limited strain at 800°C. Thermal conductivity dropped significantly for both composites at 800°C (54.55% for KF‐GPC and 59.23% for CKF‐GPC). SEM analysis revealed stronger fiber–matrix bonding and lower porosity in KF‐GPCs compared to CKF‐GPCs, which exhibited higher porosity and fiber pullout.

Zitieren

APA

Debnath, A. K., Hasib, M. A., Emon, R. A., Kafi, A. A., Fahim, T. A., & Rabbi, M. S. (2025). Physical and Thermomechanical Performance of Kevlar and Carbon–Kevlar‐Reinforced Geopolymer Composites at Elevated Temperatures. Journal of Engineering, 2025(1). https://doi.org/10.1155/je/2424227

Vancouver

Debnath AK, Hasib MA, Emon RA, Kafi AA, Fahim TA, Rabbi MS. Physical and Thermomechanical Performance of Kevlar and Carbon–Kevlar‐Reinforced Geopolymer Composites at Elevated Temperatures. Journal of Engineering. 2025;2025(1). doi:10.1155/je/2424227

BibTeX
@article{Debnath2025,
  author = {Debnath, Arup Kumar and Hasib, Md. Abdul and Emon, Rizuanul Arefin and Kafi, Abdullah Al and Fahim, Tanvir Ahmed and Rabbi, Md. Sanaul},
  title = {Physical and Thermomechanical Performance of Kevlar and Carbon–Kevlar‐Reinforced Geopolymer Composites at Elevated Temperatures},
  journal = {Journal of Engineering},
  year = {2025},
  volume = {2025},
  number = {1},
  doi = {10.1155/je/2424227}
}
Kostenlos starten →