Crystallization Behavior of CaO-SiO2-Al2O3-MgO-TiO2-FeO Slag with Different CaO/SiO2 Ratios
Materials · 2026-04-14 · 19 (8) · 1574
DOI: 10.3390/ma19081574 ↗At a glance
Journal article in Materials, published online on 2026-04-14. Written by Wu Zhu and 8 co-authors. Institution: College of Metallurgy and Energy, North China University of Science and Technology, Tangshan 063210, China. Cited 2 times so far (Crossref); 41 references. The full text is freely available (open access, CC BY 4.0). Funded by: National Key R&D Program of China, Hebei Natural Science Foundation, Central Guidance Local Science and Technology Development Fund Project of Hebei Province.
Abstract (original language)
Titanium-extracted tailing is a by-product generated during titanium-bearing blast furnace slag treatment process. The crystallization behavior of the titanium-extracted tailing during the cooling process is significant to its utilization for glass ceramics preparation. In this work, the CaO-SiO2-Al2O3-MgO-TiO2-FeO slag was used to explore the effect of CaO/SiO2 ratios on titanium-extracted tailing crystallization. FactSage 8.2 calculation and mineralogical characterizations were conducted to investigate the phase and microstructure evolution during the slag cooling process. Single hot thermocouple technique (SHTT) was employed for in situ observation of the crystallization process of the slag during the cooling process. The obtained results indicated that the perovskite, melilite, spinel, diopside and anorthite phases would be crystallized during the cooling process when the CaO/SiO2 ratios of the slag were 0.7–1.1. Increasing the CaO/SiO2 ratio to 1.3 and 1.5 promoted the crystallization of olivine and merwinite phases, however, inhibited the crystallization of diopside and anorthite phases. The initial crystallization temperature and the liquid phase disappeared temperature of the slag enhanced with improving CaO/SiO2 ratios. The initial crystallization temperature was controlled by perovskite phase precipitation when the CaO/SiO2 ratios of slag reached 0.7–1.3. Whereas the initial crystallization temperature was controlled by the crystallization of spinel phase when the CaO/SiO2 ratio of slag was 1.5. The incubation time for crystal nucleation reduced with increasing CaO/SiO2 ratios that promoted slag crystallization. Moreover, increasing the CaO/SiO2 ratio from 0.7 to 1.5 enhanced the critical cooling rate from 4 °C s−1 to 11 °C s−1.
Subjects
Author keywords
Authors and institutions
- College of Metallurgy and Energy, North China University of Science and Technology, Tangshan 063210, China.
- Hebei Puyang Iron and Steel Co., Ltd., Handan 056307, China.
- Institute of Materials Technology Research, HBIS Group Co., Ltd., Shijiazhuang 050023, China.
- Yanzhao Iron and Steel Laboratory, North China University of Science and Technology, Tangshan 063210, China.
Funding
- National Key R&D Program of China
- Hebei Natural Science Foundation
- Central Guidance Local Science and Technology Development Fund Project of Hebei Province
- S&T Program of Hebei
- Key Program of North China University of Science and Technology
- Graduate Student Innovation Foundation of North China University of Science and Technology
- North China University of Science and Technology
Cite
APA
Zhu, W., Ren, Q., Cai, S., Li, J., Li, L., Duan, L., Zeng, Y., Wang, Y., & Liu, B. (2026). Crystallization Behavior of CaO-SiO2-Al2O3-MgO-TiO2-FeO Slag with Different CaO/SiO2 Ratios. Materials, 19(8), 1574. https://doi.org/10.3390/ma19081574
Vancouver
Zhu W, Ren Q, Cai S, Li J, Li L, Duan L, et al. Crystallization Behavior of CaO-SiO2-Al2O3-MgO-TiO2-FeO Slag with Different CaO/SiO2 Ratios. Materials. 2026;19(8):1574. doi:10.3390/ma19081574
BibTeX
@article{Zhu2026,
author = {Zhu, Wu and Ren, Qianqian and Cai, Shuang and Li, Junguo and Li, Lanjie and Duan, Luyang and Zeng, Yanan and Wang, Yajun and Liu, Bao},
title = {Crystallization Behavior of CaO-SiO2-Al2O3-MgO-TiO2-FeO Slag with Different CaO/SiO2 Ratios},
journal = {Materials},
year = {2026},
volume = {19},
number = {8},
pages = {1574},
doi = {10.3390/ma19081574}
}
EUVIMED