EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Laser Power-Dependent Microstructural Evolution and Fracture Mechanisms in Ti80 Titanium Alloy Welds: A Multi-Scale Investigation

Chuanbo Zheng, Zhanwen Yang, Guo Yi, Liuyu Zhang, Xiaomeng Zhou, Xinyu Yao

Materials · 29.12.2025 · 19 (1) · 116

DOI: 10.3390/ma19010116 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 29.12.2025. Verfasst von Chuanbo Zheng und 5 weiteren Autor:innen. Beteiligte Einrichtung: School of Metallurgy and Engineering, Jiangsu University of Science and Technology, Zhangjiagang 215600, China. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 37 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The laser welding of 4 mm thick Ti80 alloy under different powers was analyzed, and the weld morphology, microstructure, and mechanical properties were studied. A simulation model was established based on ABAQUS, and laser welding simulations were conducted using 2520 W and 3000 W laser welding power sources to analyze the temperature field and stress field, which were verified by experiments. The increase in power changed the weld morphology from Y-shaped to X-shaped and affected the number of pores in incomplete and complete penetration. The microstructure in the weld zone presented fine acicular α′ phase. Subsequently, grain boundary distribution maps, Kernel Average Misorientation (KAM) maps, and geometrically necessary dislocation (GND) density maps were generated through electron backscatter diffraction (EBSD) analysis. These comprehensive data visualizations enabled multi-dimensional investigation, establishing and analyzing correlations between laser welding parameters, microstructural evolution, and mechanical properties in Ti80 titanium laser welding. The hardness of the base material was 320 HV to 360 HV, and it increased from 420 HV to 460 HV in the weld zone. At 3000 W, the tensile strength reached 903.12 MPa, and the elongation was 10.40%, indicating ductile fracture. The simulation results accurately predicted the maximum longitudinal residual stress in the weld zone, with an error of 1.65% to 1.81% of the measured value.

Schlagwörter

Stichwörter der Autor:innen

Ti80 titanium alloylaser weldingmechanical propertiessimulation

Autor:innen und Institutionen

  • School of Metallurgy and Engineering, Jiangsu University of Science and Technology, Zhangjiagang 215600, China.
  • Suzhou Sitri Welding Technology Research Institute Co., Ltd., Zhangjiagang 215600, China.

Zitieren

APA

Zheng, C., Yang, Z., Yi, G., Zhang, L., Zhou, X., & Yao, X. (2025). Laser Power-Dependent Microstructural Evolution and Fracture Mechanisms in Ti80 Titanium Alloy Welds: A Multi-Scale Investigation. Materials, 19(1), 116. https://doi.org/10.3390/ma19010116

Vancouver

Zheng C, Yang Z, Yi G, Zhang L, Zhou X, Yao X. Laser Power-Dependent Microstructural Evolution and Fracture Mechanisms in Ti80 Titanium Alloy Welds: A Multi-Scale Investigation. Materials. 2025;19(1):116. doi:10.3390/ma19010116

BibTeX
@article{Zheng2025,
  author = {Zheng, Chuanbo and Yang, Zhanwen and Yi, Guo and Zhang, Liuyu and Zhou, Xiaomeng and Yao, Xinyu},
  title = {Laser Power-Dependent Microstructural Evolution and Fracture Mechanisms in Ti80 Titanium Alloy Welds: A Multi-Scale Investigation},
  journal = {Materials},
  year = {2025},
  volume = {19},
  number = {1},
  pages = {116},
  doi = {10.3390/ma19010116}
}
Kostenlos starten →