Fachartikel in der Zeitschrift Materials, online erschienen am 12.11.2024. Verfasst von Yingchun Chen und 3 weiteren Autor:innen. Beteiligte Einrichtung: College of Architecture and Civil Engineering, Beijing University of Technology, Beijing 100124, China. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the State Administration for Market Regulation, State Administration for Market Regulation.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

High-density polyethylene (HDPE) pipelines are extensively utilized in energy transportation in the ocean. However, long-term exposure to water can alter the performance of HDPE, potentially leading to pipeline accidents. This study focuses on simulating the aging characteristics of PE100 polyethylene pipeline butt-fusion welded joints (B-FWJs) in water using hydrothermal accelerated aging experiments at various temperature gradients. The performance of the B-FWJ after hydrothermal aging was characterized using scanning electron microscopy (SEM), oxidation induction time (OIT), attenuated total reflectance Fourier transform infrared (ATR FT-IR) spectroscopy, and mechanical testing. Furthermore, this study analyzed the performance characteristics and changes in the micro-molecular chains of an HDPE B-FWJ pipeline following hydrothermal aging. An investigation was conducted into the effects of hydrothermal aging temperature and duration on the physical and chemical characteristics of HDPE B-FWJ, and the aging mechanism under hydrothermal aging conditions was explored. The results indicate that increasing hydrothermal aging temperature leads to a more significant decrease in the mechanical properties of the B-FWJ. These findings contribute to understanding the aging behavior of PE100 pipelines in the joint section and offer insights to mitigate the risks associated with the aging of and damage to B-FWJ pipelines in the ocean.

Schlagwörter

Stichwörter der Autor:innen

butt-fusion welded jointhigh-density polyethylenehydrothermal agingtemperature

Autor:innen und Institutionen

  • College of Architecture and Civil Engineering, Beijing University of Technology, Beijing 100124, China.

Förderung

  • the State Administration for Market Regulation
  • State Administration for Market Regulation

Zitieren

APA

Chen, Y., Li, Y., Yang, J., & Xi, Y. (2024). Accelerated Hydrothermal Aging and Degradation Mechanism of PE100 Butt-Fusion Welded Joint. Materials, 17(22), 5505. https://doi.org/10.3390/ma17225505

Vancouver

Chen Y, Li Y, Yang J, Xi Y. Accelerated Hydrothermal Aging and Degradation Mechanism of PE100 Butt-Fusion Welded Joint. Materials. 2024;17(22):5505. doi:10.3390/ma17225505

BibTeX
@article{Chen2024,
  author = {Chen, Yingchun and Li, Yanfeng and Yang, Jie and Xi, Yan},
  title = {Accelerated Hydrothermal Aging and Degradation Mechanism of PE100 Butt-Fusion Welded Joint},
  journal = {Materials},
  year = {2024},
  volume = {17},
  number = {22},
  pages = {5505},
  doi = {10.3390/ma17225505}
}
Kostenlos starten →