Mechanical Properties of Alkasite Material with Different Curing Modes and Simulated Aging Conditions
Materials · 06.06.2024 · 17 (11) · 2777
DOI: 10.3390/ma17112777 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 06.06.2024. Verfasst von Visnja Negovetic Mandic und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Gunduliceva 5, 10000 Zagreb, Croatia. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 50 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
This study aimed to evaluate the micro-mechanical and macro-mechanical properties of self-cured and light-cured alkasite and to investigate how accelerated degradation in acidic, alkaline, and ethanol solutions affects the macro-mechanical properties of self-cured and light-cured alkasite. The specimens of the alkasite material (Cention Forte, Ivoclar Vivadent) were prepared according to the following three curing modes: (1) light-cured immediately, (2) light-cured after a 5-min delay, and (3) self-cured. Microhardness was tested before and after immersion in absolute ethanol to indirectly determine crosslink density, while flexural strength and flexural modulus were measured using a three-point bending test after accelerated aging in the following solutions: (1) lactic acid solution (pH = 4.0), (2) NaOH solution (pH = 13.0), (3) phosphate-buffered saline solution (pH = 7.4), and (4) 75% ethanol solution. The data were statistically analyzed using a two-way ANOVA and Tukey post hoc test. The results showed that the microhardness, flexural strength, and flexural modulus were significantly lower in self-cured specimens compared to light-cured specimens. A 5-min delay between the extrusion of the material from the capsule and light curing had no significant effect on any of the measured properties. A significant effect of the accelerated aging solutions on macro-mechanical properties was observed, with ethanol and alkaline solutions having a particularly detrimental effect. In conclusion, light curing was preferable to self-curing, as it resulted in significantly better micro- and macro-mechanical properties, while a 5-min delay between mixing the capsule and light curing had no negative effects.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Gunduliceva 5, 10000 Zagreb, Croatia.
- School of Dental Medicine, University of Zagreb, Gunduliceva 5, 10000 Zagreb, Croatia.
- Department of Morphology and Anthropology, Study of Dental Medicine, School of Medicine, University of Mostar, Zrinskog Frankopana 34, 88000 Mostar, Bosnia and Herzegovina.
ORCID-Profile: Visnja Negovetic Mandic, Laura Plancak, Danijela Marovic, Milena Trutina Gavran, Matej Par
Zitieren
APA
Negovetic Mandic, V., Plancak, L., Marovic, D., Tarle, Z., Trutina Gavran, M., & Par, M. (2024). Mechanical Properties of Alkasite Material with Different Curing Modes and Simulated Aging Conditions. Materials, 17(11), 2777. https://doi.org/10.3390/ma17112777
Vancouver
Negovetic Mandic V, Plancak L, Marovic D, Tarle Z, Trutina Gavran M, Par M. Mechanical Properties of Alkasite Material with Different Curing Modes and Simulated Aging Conditions. Materials. 2024;17(11):2777. doi:10.3390/ma17112777
BibTeX
@article{NegoveticMandic2024,
author = {Negovetic Mandic, Visnja and Plancak, Laura and Marovic, Danijela and Tarle, Zrinka and Trutina Gavran, Milena and Par, Matej},
title = {Mechanical Properties of Alkasite Material with Different Curing Modes and Simulated Aging Conditions},
journal = {Materials},
year = {2024},
volume = {17},
number = {11},
pages = {2777},
doi = {10.3390/ma17112777}
}
EUVIMED