EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

The Effect of Restoration Thickness on the Fracture Resistance of 5 mol% Yttria-Containing Zirconia Crowns

Po-Hsu Chen iD, Esra Elamin, Akram Sayed Ahmed iD, Daniel A Givan, Chin-Chuan Fu, Nathaniel C Lawson iD

Materials · 11.01.2024 · 17 (2) · 365

DOI: 10.3390/ma17020365 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 11.01.2024. Verfasst von Po-Hsu Chen und 5 weiteren Autor:innen. Beteiligte Einrichtung: Division of Prosthodontics, University of Alabama at Birmingham School of Dentistry, Birmingham, AL 35209, USA. Die Arbeit wurde bisher 7-mal zitiert (Crossref) und nennt 41 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Background

To determine what thickness of 5 mol% yttria zirconia (5Y-Z) translucent crowns cemented with different cements and surface treatments would have equivalent fracture resistance as 3 mol% yttria (3Y-Z) crowns.

Methods

The study included 0.8 mm, 1.0 mm, and 1.2 mm thickness 5Y-Z (Katana UTML) crowns and 0.5 and 1.0 mm thickness 3Y-Z (Katana HT) crowns as controls. The 5Y-Z crowns were divided among three treatment subgroups (n = 10/subgroup): (1) cemented using RMGIC (Rely X Luting Cement), (2) alumina particle-abraded then luted with the same cement, (3) alumina particle-abraded and cemented using a resin cement (Panavia SA Cement Universal). The 3Y-Z controls were alumina particle-abraded then cemented with RMGIC. The specimens were then loaded in compression at 30° until failure.

Results

All 5Y-Z crowns (regardless of thickness or surface treatment) had a similar to or higher fracture force than the 0.5 mm 3Y-Z crowns. Only the 1.2 mm 5Y-Z crowns with resin cement showed significantly similar fracture force to the 1 mm 3Y-Z crowns.

Conclusion

In order to achieve a similar fracture resistance to 0.5 mm 3Y-Z crowns cemented with RMGIC, 5Y-Z crowns may be as thin as 0.8 mm. To achieve a similar fracture resistance to 1.0 mm 3Y-Z crowns cemented with RMGIC, 5Y-Z crowns must be 1.2 mm and bonded with resin cement.

Schlagwörter

Stichwörter der Autor:innen

cementationcrown fracturezirconia

Autor:innen und Institutionen

  • Division of Prosthodontics, University of Alabama at Birmingham School of Dentistry, Birmingham, AL 35209, USA.
  • Faculty of Dentistry, Department of Dental Biomaterials, Tanta University, Tanta 31527, Egypt.

ORCID-Profile: Po-Hsu Chen, Akram Sayed Ahmed, Nathaniel C Lawson

Zitieren

APA

Chen, P. H., Elamin, E., Sayed Ahmed, A., Givan, D. A., Fu, C. C., & Lawson, N. C. (2024). The Effect of Restoration Thickness on the Fracture Resistance of 5 mol% Yttria-Containing Zirconia Crowns. Materials, 17(2), 365. https://doi.org/10.3390/ma17020365

Vancouver

Chen PH, Elamin E, Sayed Ahmed A, Givan DA, Fu CC, Lawson NC. The Effect of Restoration Thickness on the Fracture Resistance of 5 mol% Yttria-Containing Zirconia Crowns. Materials. 2024;17(2):365. doi:10.3390/ma17020365

BibTeX
@article{Chen2024,
  author = {Chen, Po-Hsu and Elamin, Esra and Sayed Ahmed, Akram and Givan, Daniel A and Fu, Chin-Chuan and Lawson, Nathaniel C},
  title = {The Effect of Restoration Thickness on the Fracture Resistance of 5 mol% Yttria-Containing Zirconia Crowns},
  journal = {Materials},
  year = {2024},
  volume = {17},
  number = {2},
  pages = {365},
  doi = {10.3390/ma17020365}
}
Kostenlos starten →