Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 18.04.2023. Verfasst von Baofeng Zhang und 6 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Engineering, Huanghe Science and Technology College, Zhengzhou 450063, China. Die Arbeit wurde bisher 22-mal zitiert (Crossref) und nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Key scientific research project plan of colleges and universities in Henan Province, Doctoral Training Fund of Henan University of Engineering, Henan Province Science and Technology Research Plan Project.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

CoCrCuFeMnNix (x = 0, 0.5, 1.0, 1.5, 2.0 mol, named as Ni0, Ni0.5, Ni1.0, Ni1.5, and Ni2.0, respectively) high-entropy alloy powders (HEAPs) were prepared via mechanical alloying (MA), and XRD, SEM, EDS, and vacuum annealing were used to study the alloying behavior, phase transition, and thermal stability. The results indicated that the Ni0, Ni0.5, and Ni1.0 HEAPs were alloyed at the initial stage (5–15 h), the metastable BCC + FCC two-phase solid solution structure was formed, and the BCC phase disappeared gradually with the prolonging of ball milling time. Finally, a single FCC structure was formed. Both Ni1.5 and Ni2.0 alloys with high nickel content formed a single FCC structure during the whole mechanical alloying process. The five kinds of HEAPs showed equiaxed particles in dry milling, and the particle size increased with an increase in milling time. After wet milling, they changed into lamellar morphology with thickness less than 1 μm and maximum size less than 20 μm. The composition of each component was close to its nominal composition, and the alloying sequence during ball milling was Cu→Mn→Co→Ni→Fe→Cr. After vacuum annealing at 700~900 °C, the FCC phase in the HEAPs with low Ni content transformed into FCC2 secondary phase, FCC1 primary phase, and a minor σ phase. The thermal stability of HEAPs can be improved by increasing Ni content.

Schlagwörter

Stichwörter der Autor:innen

high-entropy alloy powdermechanical alloyingphase transitionthermal stabilityvacuum annealing

Autor:innen und Institutionen

  • Faculty of Engineering, Huanghe Science and Technology College, Zhengzhou 450063, China.
  • School of Mechanical Engineering, Henan University of Engineering, Zhengzhou 451191, China.

ORCID-Profile: Bo Ren

Förderung

  • Key scientific research project plan of colleges and universities in Henan Province
  • Doctoral Training Fund of Henan University of Engineering
  • Henan Province Science and Technology Research Plan Project

Zitieren

APA

Zhang, B., Zhao, R., Ren, B., Jiang, A., Chen, C., Liu, J., & Zhou, Y. (2023). Mechanical Alloying Behavior and Thermal Stability of CoCrCuFeMnNix High-Entropy Alloy Powders Prepared via MA. Materials, 16(8), 3179. https://doi.org/10.3390/ma16083179

Vancouver

Zhang B, Zhao R, Ren B, Jiang A, Chen C, Liu J, et al. Mechanical Alloying Behavior and Thermal Stability of CoCrCuFeMnNix High-Entropy Alloy Powders Prepared via MA. Materials. 2023;16(8):3179. doi:10.3390/ma16083179

BibTeX
@article{Zhang2023,
  author = {Zhang, Baofeng and Zhao, Ruifeng and Ren, Bo and Jiang, Aiyun and Chen, Chong and Liu, Jianxiu and Zhou, Yajun},
  title = {Mechanical Alloying Behavior and Thermal Stability of CoCrCuFeMnNix High-Entropy Alloy Powders Prepared via MA},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {8},
  pages = {3179},
  doi = {10.3390/ma16083179}
}
Kostenlos starten →