Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 23.03.2023. Verfasst von Michal Wieczorowski und 4 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Mechanical Engineering, Poznan University of Technology, Piotrowo Street 3, 60-965 Poznan, Poland. Die Arbeit wurde bisher 56-mal zitiert (Crossref) und nennt 53 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: ITA company, Erasmus Program under the agreement between Poznand University of Technology and Universidade de Vigo.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Wire arc additive manufacturing (WAAM) is renowned for its high deposition rate, enabling the production of large parts. However, the process has challenges such as porosity formation, residual stresses, and cracking when manufacturing aluminum parts. This study focuses on ana-lyzing the porosity of AA5356 walls manufactured using the WAAM process with the Fronius cold metal transfer system (Wels, Austria). The walls were machined to obtain specimens for tensile testing. The study used computed tomography and the tensile test to analyze the specimens’ porosity and its potential relation to tensile strength. The process parameters analyzed were travel speed, cooling time, and path strategy. In conclusion, increasing travel speed and cooling time significantly affects pore diameter due to the lower heat input to the weld zone. Porosity can be reduced when diminishing heat accumulation. The results indicate that an increase in travel speed produces a slight decrease in porosity. Specifically, the total pore volume diminishes from 0.42 to 0.36 mm3 when increasing the travel speed from 700 to 950 mm/min. The ultimate tensile strength and maximum elongation of the ‘back and forth’ strategy are slightly higher than those of the ‘go’ strategy. After tensile testing, the ultimate tensile strength and yield strength did not show any relation to the porosity measured by computed tomography. The percentage of the pore total volume over the measured volume was lower than 0.12% for all the scanned specimens.

Schlagwörter

Stichwörter der Autor:innen

AA5356WAAMadditive manufacturingcomputed tomographymulti-layered wallstensile testing

Autor:innen und Institutionen

  • Faculty of Mechanical Engineering, Poznan University of Technology, Piotrowo Street 3, 60-965 Poznan, Poland.
  • Escola de Enxeñaría Industrial, Campus Lagoas Marcosende, Universidade de Vigo, 36310 Vigo, Spain.
  • Escola de Enxeñaría Aeronáutica e do Espazo, Universidade de Vigo, 32004 Ourense, Spain.

ORCID-Profile: Michal Wieczorowski, Alejandro Pereira, Diego Carou, Bartosz Gapinski

Förderung

  • ITA company
  • Erasmus Program under the agreement between Poznand University of Technology and Universidade de Vigo

Zitieren

APA

Wieczorowski, M., Pereira, A., Carou, D., Gapinski, B., & Ramírez, I. (2023). Characterization of 5356 Aluminum Walls Produced by Wire Arc Additive Manufacturing (WAAM). Materials, 16(7), 2570. https://doi.org/10.3390/ma16072570

Vancouver

Wieczorowski M, Pereira A, Carou D, Gapinski B, Ramírez I. Characterization of 5356 Aluminum Walls Produced by Wire Arc Additive Manufacturing (WAAM). Materials. 2023;16(7):2570. doi:10.3390/ma16072570

BibTeX
@article{Wieczorowski2023,
  author = {Wieczorowski, Michal and Pereira, Alejandro and Carou, Diego and Gapinski, Bartosz and Ramírez, Ignacio},
  title = {Characterization of 5356 Aluminum Walls Produced by Wire Arc Additive Manufacturing (WAAM)},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {7},
  pages = {2570},
  doi = {10.3390/ma16072570}
}