EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Consolidation of Tantalum Powders by Spark Plasma Sintering: Densification, Wear and Corrosion Behavior

Elena Mihalcea, Jorge Chávez, Omar Jiménez, Martín Flores, Francisco Alvarado-Hernández, Juan Pablo Camarillo-García, Horacio Flores-Zúñiga, Marco Aurelio González-Albarrán, Luis Olmos

Lubricants · 21.07.2026 · 14 (7) · 280

DOI: 10.3390/lubricants14070280 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Lubricants, online erschienen am 21.07.2026. Verfasst von Elena Mihalcea und 8 weiteren Autor:innen. Die Arbeit nennt 57 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Tantalum (Ta) is an excellent alternative for structural orthopedic implants because of its high biocompatibility and chemical stability, but its melting point of 3020 °C severely complicates conventional casting. To address this, the study evaluates spark plasma sintering (SPS) to consolidate pure Ta powders at 1450 °C and 50 MPa and analyzes the impact of heating rates (50–200 °C/min) on microstructural, mechanical, wear, and corrosion properties. Results indicate that heating rate dictates final densification: a 50 °C/min rate achieved 98.59% relative density, whereas 200 °C/min yielded only 82.28% due to reduced thermal exposure. Sintering involved dislocation creep and viscous flow mechanisms, with X-ray diffraction confirming a stable α-Ta matrix across all samples. Mechanically, the 50 °C/min samples achieved a maximum microhardness of 285 HV, whereas higher porosity at 200 °C/min reduced hardness by 27.8%. Wear testing showed a two-stage friction evolution: an initial Ta2O5 solid-lubricating effect, followed by predominant abrasion and adhesion, with stable wear rates (3.2 to 3.6 × 10−3 mm3/N·m) for dense specimens. Finally, tests in simulated body fluid confirmed spontaneous self-passivation. However, the corrosion rate increased with heating rates, indicating that the resulting porosity adversely affects the material’s surface response.

Zitieren

APA

Mihalcea, E., Chávez, J., Jiménez, O., Flores, M., Alvarado-Hernández, F., Camarillo-García, J. P., Flores-Zúñiga, H., González-Albarrán, M. A., & Olmos, L. (2026). Consolidation of Tantalum Powders by Spark Plasma Sintering: Densification, Wear and Corrosion Behavior. Lubricants, 14(7), 280. https://doi.org/10.3390/lubricants14070280

Vancouver

Mihalcea E, Chávez J, Jiménez O, Flores M, Alvarado-Hernández F, Camarillo-García JP, et al. Consolidation of Tantalum Powders by Spark Plasma Sintering: Densification, Wear and Corrosion Behavior. Lubricants. 2026;14(7):280. doi:10.3390/lubricants14070280

BibTeX
@article{Mihalcea2026,
  author = {Mihalcea, Elena and Chávez, Jorge and Jiménez, Omar and Flores, Martín and Alvarado-Hernández, Francisco and Camarillo-García, Juan Pablo and Flores-Zúñiga, Horacio and González-Albarrán, Marco Aurelio and Olmos, Luis},
  title = {Consolidation of Tantalum Powders by Spark Plasma Sintering: Densification, Wear and Corrosion Behavior},
  journal = {Lubricants},
  year = {2026},
  volume = {14},
  number = {7},
  pages = {280},
  doi = {10.3390/lubricants14070280}
}
Kostenlos starten →