Optimizing the Die-Sink EDM Machinability of AISI 316L Using Ti-6Al-4V-SiCp Electrodes: A Computational Approach
Journal of Manufacturing and Materials Processing · 18.09.2024 · 8 (5) · 202
DOI: 10.3390/jmmp8050202 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Manufacturing and Materials Processing, online erschienen am 18.09.2024. Verfasst von Adithya Hegde und 4 weiteren Autor:innen. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 65 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Die-sink electric discharge machining (EDM) is essential for shaping complex geometries in hard-to-machine materials. This study aimed to optimize key input parameters, such as the discharge current, gap voltage, pulse-on time, and pulse-off time, to enhance the EDM performance by maximizing the material removal rate while minimizing the surface roughness, residual stress, microhardness, and recast layer thickness. AISI 316L stainless steel was chosen due to its industrial relevance and machining challenges, while a Ti-6Al-4V-SiCp composite electrode was selected for its thermal resistance and low wear. Using Taguchi’s L27 orthogonal array, this study minimized the trial numbers, with analysis of the variance-quantifying parameter contributions. The results showed a maximum material removal rate of 0.405 g/min and minimal values for the surface roughness (1.95 µm), residual stress (1063.74 MPa), microhardness (244.8 Hv), and recast layer thickness (0.47 µm). A second-order model, developed through a response surface methodology, and a feed-forward artificial neural network enhanced the prediction accuracy. Multi-response optimization using desirability function analysis yielded an optimal set of conditions: discharge current of 5.78 amperes, gap voltage of 90 volts, pulse-on time of 100 microseconds, and pulse-off time of 15 microseconds. This setup achieved a material removal rate of 0.13 g/min, with reduced surface roughness (2.46 µm), residual stress (1518.46 MPa), microhardness (259.01 Hv), and recast layer thickness (0.87 µm). Scanning electron microscopy further analyzed the surface morphology and recast layer characteristics, providing insights into the material behavior under EDM. These findings enhance the understanding and optimization of the EDM processes for challenging materials, offering valuable guidance for future research and industrial use.
Zitieren
APA
Hegde, A., Shetty, R., Nayak, R., Shetty, S., & SV, U. K. S. (2024). Optimizing the Die-Sink EDM Machinability of AISI 316L Using Ti-6Al-4V-SiCp Electrodes: A Computational Approach. Journal of Manufacturing and Materials Processing, 8(5), 202. https://doi.org/10.3390/jmmp8050202
Vancouver
Hegde A, Shetty R, Nayak R, Shetty S, SV UKS. Optimizing the Die-Sink EDM Machinability of AISI 316L Using Ti-6Al-4V-SiCp Electrodes: A Computational Approach. Journal of Manufacturing and Materials Processing. 2024;8(5):202. doi:10.3390/jmmp8050202
BibTeX
@article{Hegde2024,
author = {Hegde, Adithya and Shetty, Raviraj and Nayak, Rajesh and Shetty, Sawan and SV, Uday Kumar Shetty},
title = {Optimizing the Die-Sink EDM Machinability of AISI 316L Using Ti-6Al-4V-SiCp Electrodes: A Computational Approach},
journal = {Journal of Manufacturing and Materials Processing},
year = {2024},
volume = {8},
number = {5},
pages = {202},
doi = {10.3390/jmmp8050202}
}
EUVIMED