EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of Ceramic-Media Tumbling Duration on the Surface Characteristics and Corrosion Behavior of SLM-Manufactured AISI 316L Stainless Steel Under Simulated Microbial-Induced Corrosion Conditions

Josef Hlinka, Renata Palupcikova, Vlastimil Vodarek, Jirina Vontorova, Jiri Hajnys, Jakub Mesicek, Petr Sotnar, Michal Kresta, Tomas Kohut, Nadimul Haque Faisal

Journal of Manufacturing and Materials Processing · 03.11.2026 · 10 (11) · 483

DOI: 10.3390/jmmp10110483 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Manufacturing and Materials Processing, online erschienen am 03.11.2026. Verfasst von Josef Hlinka und 9 weiteren Autor:innen. Die Arbeit nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Comprehensive evaluation of the influence of production and processing technologies and degradation mechanisms on the properties of structural materials, European Union.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Surface finishing of SLM-manufactured AISI 316L aims to reduce recessed features that may retain deposits and create occluded corrosion environments. This study evaluates whether extending ceramic-media tumbling provides electrochemical benefits beyond initial surface smoothing. An as-built reference and specimens tumbled for 30–120 min were characterized using Ra, Rz, Sa, and Sz, confocal microscopy, SEM, metallographic cross-sections, and wettability measurements. Electrochemical impedance spectroscopy and potentiodynamic polarization were performed after 100 h in 0.1 M H2SO4, an abiotic surrogate for acidification associated with sulfur-oxidizing microorganisms. After 120 min, Ra and Rz decreased from 7.2 and 32.2 to 1.9 and 11.0 µm, while Sa and Sz decreased from 21.1 and 216.9 to 8.9 and 102.2 µm, respectively. The Tafel-derived corrosion rate decreased from 9.8 to 2.5 µm year−1, and the Stern–Geary polarization resistance increased from 32 to 68 kΩ cm2. The largest profile roughness reductions occurred during the first 30 min, whereas the polarization results showed limited additional improvement between 90 and 120 min. The impedance modulus at 0.1 Hz varied non-monotonically. The combined assessment reveals different duration-dependent topographical and electrochemical responses, supporting evaluation of finishing duration using both. Effects on microbial colonization require further biological validation.

Förderung

  • Comprehensive evaluation of the influence of production and processing technologies and degradation mechanisms on the properties of structural materials
  • European Union

Zitieren

APA

Hlinka, J., Palupcikova, R., Vodarek, V., Vontorova, J., Hajnys, J., Mesicek, J., Sotnar, P., Kresta, M., Kohut, T., & Faisal, N. H. (2026). Effect of Ceramic-Media Tumbling Duration on the Surface Characteristics and Corrosion Behavior of SLM-Manufactured AISI 316L Stainless Steel Under Simulated Microbial-Induced Corrosion Conditions. Journal of Manufacturing and Materials Processing, 10(11), 483. https://doi.org/10.3390/jmmp10110483

Vancouver

Hlinka J, Palupcikova R, Vodarek V, Vontorova J, Hajnys J, Mesicek J, et al. Effect of Ceramic-Media Tumbling Duration on the Surface Characteristics and Corrosion Behavior of SLM-Manufactured AISI 316L Stainless Steel Under Simulated Microbial-Induced Corrosion Conditions. Journal of Manufacturing and Materials Processing. 2026;10(11):483. doi:10.3390/jmmp10110483

BibTeX
@article{Hlinka2026,
  author = {Hlinka, Josef and Palupcikova, Renata and Vodarek, Vlastimil and Vontorova, Jirina and Hajnys, Jiri and Mesicek, Jakub and Sotnar, Petr and Kresta, Michal and Kohut, Tomas and Faisal, Nadimul Haque},
  title = {Effect of Ceramic-Media Tumbling Duration on the Surface Characteristics and Corrosion Behavior of SLM-Manufactured AISI 316L Stainless Steel Under Simulated Microbial-Induced Corrosion Conditions},
  journal = {Journal of Manufacturing and Materials Processing},
  year = {2026},
  volume = {10},
  number = {11},
  pages = {483},
  doi = {10.3390/jmmp10110483}
}
Kostenlos starten →