Effect of Fe and Thermal Exposure on Mechanical Properties of Al-Si-Cu-Ni-Mg-Fe Alloy

Jingdong Li, Fanming Chen, Yuze Wang, Yuanliang Zhang, Rui Zhang, Yi Luo, Yiqiang He, Ke Sun, Lijie Zuo

Crystals · 21.06.2023 · 13 (7) · 993

DOI: 10.3390/cryst13070993 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Crystals, online erschienen am 21.06.2023. Verfasst von Jingdong Li und 8 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 21 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Natural Science Foundation of the Jiangsu Higher Education Institutions of China, Jiangsu Institute of Marine Resources Development, Jiangsu Province Special Project for the Transformation of Scientific and Technological Achievements.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The effects of Fe, Cr and thermal exposure on the microstructure and mechanical properties of Al-Si alloy were investigated in this work. The results indicated that the main phases of the Al-Si-Cu-Ni-Mg-(0.6–0.9%) Fe (wt. %) alloy were α-Al, Si, Al5Cu2Mg8Si6, Al3CuNi, Al7Cu4Ni, Al2Cu, and AlFeSi at room temperature. The size of the AlSiFe phase increased with increasing the weight fraction of Fe. The shape of Fe-rich phase changed from rod-like to star-like, followed by long needle-like with Fe varying from 0.6% to 0.9%. The mechanical properties of the studied alloys at elevated temperatures increased with Fe. The ultimate tensile strength of the three alloys at 350 °C was 111.2 MPa, 124 MPa, and 128.7 MPa, respectively. In addition, the ductility and strength of the studied alloys at room temperature decreased with increasing the Fe, due to the large size of the hard and brittle Fe-rich phase strictly cleaved the aluminum matrix. After thermal exposure, the properties of the alloy at room temperature and elevated temperature decreased obviously at the beginning of 0.5~8 h, and then tend to be stabilized during thermal exposure at 350 °C for approximately 32~64 h. Fe-rich was a thermal stable phase at 350 °C.

Förderung

  • Natural Science Foundation of the Jiangsu Higher Education Institutions of China
  • Jiangsu Institute of Marine Resources Development
  • Jiangsu Province Special Project for the Transformation of Scientific and Technological Achievements

Zitieren

APA

Li, J., Chen, F., Wang, Y., Zhang, Y., Zhang, R., Luo, Y., He, Y., Sun, K., & Zuo, L. (2023). Effect of Fe and Thermal Exposure on Mechanical Properties of Al-Si-Cu-Ni-Mg-Fe Alloy. Crystals, 13(7), 993. https://doi.org/10.3390/cryst13070993

Vancouver

Li J, Chen F, Wang Y, Zhang Y, Zhang R, Luo Y, et al. Effect of Fe and Thermal Exposure on Mechanical Properties of Al-Si-Cu-Ni-Mg-Fe Alloy. Crystals. 2023;13(7):993. doi:10.3390/cryst13070993

BibTeX
@article{Li2023,
  author = {Li, Jingdong and Chen, Fanming and Wang, Yuze and Zhang, Yuanliang and Zhang, Rui and Luo, Yi and He, Yiqiang and Sun, Ke and Zuo, Lijie},
  title = {Effect of Fe and Thermal Exposure on Mechanical Properties of Al-Si-Cu-Ni-Mg-Fe Alloy},
  journal = {Crystals},
  year = {2023},
  volume = {13},
  number = {7},
  pages = {993},
  doi = {10.3390/cryst13070993}
}
Kostenlos starten →