Fachartikel in der Zeitschrift Coatings, online erschienen am 09.03.2026. Verfasst von Huabing Yang und 10 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Shandong Province Key Research and Development Plan, National Natural Science Foundation of China, Major Innovation Project for integrating Science, Education & Industry of Qilu University of Technology.
Abstract (Originalsprache)
It is well known that residual stress is detrimental to mechanical properties of metal materials. This paper investigated the relief of residual stress during long-time natural aging as well as its influence on tensile properties of partial age-hardenable Al alloys. It was found that uniform elongation and ultimate tensile stress were increased after a long-time natural aging of T6 heat-treated 2024, A356, 6063 and 6061 alloys. For example, uniform elongation and ultimate tensile stress of 2024 alloy were respectively increased from 10.2% and 496.7 MPa to 11.1% and 507.5 MPa. According to fracture behavior observation for 2024 and A356 alloys, cracks or/and voids could generate from micron-sized secondary particles or particle/α-Al interface in matrix, which led to fracture of tensile samples eventually. And reduced residual stress during natural aging delayed formation of the cracks or voids based on stress distribution analysis, which led to an increase in uniform elongation and tensile stress of Al alloys.
Förderung
- Shandong Province Key Research and Development Plan
- National Natural Science Foundation of China
- Major Innovation Project for integrating Science, Education & Industry of Qilu University of Technology
- Natural Science Foundation of Shandong Province
Zitieren
APA
Yang, H., Chen, H., Cheng, K., Qiao, Z., Wang, X., Wu, J., Zhao, D., Feng, X., Wang, J., Cheng, K., & Zhou, J. (2026). Influence of Natural Aging After T6 Heat Treatment on Mechanical Properties of Age-Hardenable Al Alloys. Coatings, 16(3), 339. https://doi.org/10.3390/coatings16030339
Vancouver
Yang H, Chen H, Cheng K, Qiao Z, Wang X, Wu J, et al. Influence of Natural Aging After T6 Heat Treatment on Mechanical Properties of Age-Hardenable Al Alloys. Coatings. 2026;16(3):339. doi:10.3390/coatings16030339
BibTeX
@article{Yang2026,
author = {Yang, Huabing and Chen, Haiyuan and Cheng, Kai and Qiao, Zhiyao and Wang, Xitao and Wu, Jianhua and Zhao, Dongqing and Feng, Xuansheng and Wang, Jin and Cheng, Kaiming and Zhou, Jixue},
title = {Influence of Natural Aging After T6 Heat Treatment on Mechanical Properties of Age-Hardenable Al Alloys},
journal = {Coatings},
year = {2026},
volume = {16},
number = {3},
pages = {339},
doi = {10.3390/coatings16030339}
}
EUVIMED