Influence of Ni on the Microstructures and Mechanical Properties of Heat-Treated Al-Cu-Ce-Mn-Zr Alloys
Crystals · 23.02.2023 · 13 (3) · 380
DOI: 10.3390/cryst13030380 ↗Kurz gefasst
Fachartikel in der Zeitschrift Crystals, online erschienen am 23.02.2023. Verfasst von Xiang Su und 8 weiteren Autor:innen. Die Arbeit wurde bisher 15-mal zitiert (Crossref) und nennt 72 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of the Jiangsu Higher Education Institutions of China, Natural Science Foundation of Jiangsu Province.
Abstract (Originalsprache)
In order to enhance the high-temperature mechanical performance to meet service requirements, the microstructures and tensile properties of heat-treated Al-8.4Cu-2.3Ce-1.0Mn-0.2Zr-xNi (x = 0, 0.5, 1.0, 2.0, 4.0 wt.%) were investigated. The metallographic analysis techniques have been used to examine the microstructural changes with different Ni contents. Results show that after adding 0.5% Ni to the Al-8.4Cu-2.3Ce-1.0Mn-0.2Zr alloy, the spheroidized Al7Cu4Ni phase is formed. With Ni content further increasing, the Al8CeCu4 and Al24MnCu8Ce3 phases disappear, and the nano-sized Al20Cu2Mn3 and Al2Cu phases decrease gradually. When Ni content reaches 4.0%, the Al3CuNi phase appears. It turns out that the addition of 0.5% Ni has significantly improved the tensile properties at 400 °C. The ultimate tensile strength, yield strength, and elongation of Al-8.4Cu-2.3Ce-1.0Mn-0.2Zr-0.5Ni alloy at 400 °C reach 103 MPa, 93 Mpa, and 18.0%, respectively, which makes the alloy possible to be employed at 400 °C. The intermetallic micro-skeleton, composed of thermostable Al8CeCu4, Al24MnCu8Ce3, Al16Cu4Mn2Ce, and Al7Cu4Ni phases at the grain boundaries as well as nano-sized Al20Cu2Mn3 and Al2Cu precipitates in the grains, contributes to the good elevated-temperature tensile strength. The fracture mechanism is changed from quasi-cleavage at ambient temperature to coexistence of quasi-cleavage and dimple at 400 °C.
Förderung
- National Natural Science Foundation of China
- Natural Science Foundation of the Jiangsu Higher Education Institutions of China
- Natural Science Foundation of Jiangsu Province
- Jiangsu Province Industry-University-Research Cooperation Project
Zitieren
APA
Su, X., Qu, H., Lei, Y., Hou, R., Cao, Y., Siddique, S., Qi, Z., Shen, G., & Fan, X. (2023). Influence of Ni on the Microstructures and Mechanical Properties of Heat-Treated Al-Cu-Ce-Mn-Zr Alloys. Crystals, 13(3), 380. https://doi.org/10.3390/cryst13030380
Vancouver
Su X, Qu H, Lei Y, Hou R, Cao Y, Siddique S, et al. Influence of Ni on the Microstructures and Mechanical Properties of Heat-Treated Al-Cu-Ce-Mn-Zr Alloys. Crystals. 2023;13(3):380. doi:10.3390/cryst13030380
BibTeX
@article{Su2023,
author = {Su, Xiang and Qu, Hongjie and Lei, Yuan and Hou, Rui and Cao, Yuede and Siddique, Suniya and Qi, Zhixiang and Shen, Guoyan and Fan, Xueyi},
title = {Influence of Ni on the Microstructures and Mechanical Properties of Heat-Treated Al-Cu-Ce-Mn-Zr Alloys},
journal = {Crystals},
year = {2023},
volume = {13},
number = {3},
pages = {380},
doi = {10.3390/cryst13030380}
}
EUVIMED